Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 190 - 218 °C | 374 - 424 °F | blown film equipment |
DuPont Nucrel® 0903HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 9 wt% Methacrylic Acid.Nucrel® 0903HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment design.. |
|||
Melt Temperature | 190 - 218 °C | 374 - 424 °F | blown film equipment |
DuPont Nucrel® 0902HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 9 wt% Methacrylic Acid.Nucrel® 0902HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment design.. |
|||
Melt Temperature | 175 - 218 °C | 347 - 425 °F | Average value: 194 °C Grade Count:62 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |