Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 160 - 200 °C | 320 - 392 °F | |
PolyOne OnFlex™ U 5470A-E0083 Thermoplastic Elastomer (TPE) OnFlex™-U thermoplastic elastomer compounds are based on thermoplastic polyurethane elastomers (TPE-U). The OnFlex™-U 5400 series are based upon alloys of SEBS and aliphatic TPU, combining the adv.. |
|||
Melt Temperature | 180 - 200 °C | 356 - 392 °F | |
Lotte Chemical Titan TITANEX® LF1043 Linear low density polyethylene resin
(discontinued **) LF1043 is a pelleted linear low density polyethylene resin formulated with antioxidant, and antiblock agent. This product is used for blown film extrusion which offers outstanding toughness, extrud.. |
|||
Melt Temperature | 180 - 200 °C | 356 - 392 °F | |
Lotte Chemical Titan TITANEX® LF1051 Linear low density polyethylene Hexene-1 resin
(discontinued **) LF1051 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant, high antiblock and slip agent. This product is used for blown film extrusion which offers outstandin.. |
|||
Melt Temperature | 180 - 200 °C | 356 - 392 °F | |
Lotte Chemical Titan TITANEX® LF1054 Linear low density polyethylene Hexene-1 resin
(discontinued **) LF1054 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding toughness, extrudability and .. |
|||
Melt Temperature | 180 - 200 °C | 356 - 392 °F | |
Lotte Chemical Titan TITANCEED® mL1064 Linear low density polyethylene resin
(discontinued **) Titanceed® mL1064 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL1064 have outstanding tensile, impact and puncture stre.. |
|||
Melt Temperature | 180 - 200 °C | 356 - 392 °F | |
LATI LATILUB 73/13-01M Polyoxymethylene Base (POM), 1% Molybdenum Disulfide Self Lubricating Plastic
(Unv Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Melt Temperature | 160 - 200 °C | 320 - 392 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 10288D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Temperature | 190 - 200 °C | 374 - 392 °F | |
LG Chemical LUCEL FW-715C Friction and Wear Resistant POM, Polymeric Wear Additive, CaCo3 Filled, Low Warpage, Antistatic LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Melt Temperature | 190 - 200 °C | 374 - 392 °F | |
LG Chemical LUCEL N115 POM, Unreinforced, High Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Melt Temperature | 180 - 200 °C | 356 - 392 °F | |
LATI Latene® EP 7-V2HF PP Copolymer, Flame Retardant Polypropylene copolymer (PPc) based compound. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; N.. |
|||
Melt Temperature | 150 - 200 °C | 302 - 392 °F | Injection Molding |
Stellarchem LP-870 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Melt Temperature | 150 - 200 °C | 302 - 392 °F | Injection Molding |
Stellarchem MP-845B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Melt Temperature | 160 - 200 °C | 320 - 392 °F | Injection Molding |
Stellarchem SV-B65E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Melt Temperature | 180 - 200 °C | 356 - 392 °F | |
Eurostar Star L POM D11 POM, Injection Molded Star L POM D11 is Silicone Oil Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 180 - 200 °C | 356 - 392 °F | |
Eurostar Star L POM D51 POM, Injection Molded Star L POM D51 is a PTFE Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 180 - 200 °C | 356 - 392 °F | |
LATI Latimass 47/7-04 D008 PP Copolymer Specific density compound based on Polypropylene copolymer (PPc). Special filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati In.. |