Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Polymer Resources PC-BR1 Polycarbonate, Branched for Extrusion and Blow Molding Polycarbonate, Branched for Extrusion and Blow MoldingFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical and thermal te.. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Polymer Resources PC-BR1-UV Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilized Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilizedFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical.. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Polymer Resources PC-FR1A-D Polycarbonate, Flame Retardant, Low Flow Polycarbonate, Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing co.. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Polymer Resources PC-GP1-10TFE Polycarbonate, General Purpose, Wear Resistant, Low Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Polymer Resources PC-GP1-TFE5 Polycarbonate, 5% PTFE, Wear Resistant, Low Flow Polycarbonate, 5% PTFE, General Purpose, Wear Resistant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Melt Temperature | 316 - 321 °C | 601 - 610 °F | |
LNP Lubricomp® OFL-4036 Polyphenylene Sulfide, Glass Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Melt Temperature | 316 - 321 °C | 601 - 610 °F | |
LNP Lubricomp® OFL-4536 Polyphenylene Sulfide, Glass Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Melt Temperature | 316 - 321 °C | 601 - 610 °F | |
LNP Thermotuf® OF-1006 HI Polyphenylene Sulfide, Glass Fiber Reinforcement
(discontinued **) Features: High Impact ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades .. |
|||
Melt Temperature | 316 - 329 °C | 601 - 624 °F | |
LNP Thermocomp® UC-1006 Polyphthalamide, Carbon Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Melt Temperature | 316 - 329 °C | 601 - 624 °F | |
LNP Thermocomp® UF-1006 HS Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Polymer Resources PC-FD1 Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Polymer Resources PC-FR1-D-[color]-3 Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
PTS Tristar® PC-10R-CL(6) 6 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 316 °C | 601 °F | |
LNP Thermocomp® FP-EC-1004 Ethylene Tetrafluoroethylene Copolymer, Carbon Fiber Reinforcement
(discontinued * Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Melt Temperature | 316 - 371 °C | 601 - 700 °F | |
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU)
(Unverified Data**) Udel polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel P-3500 LCD MB series polymers are particularly well suited for the fabrication of porous .. |
|||
Melt Temperature | 316 - 343 °C | 601 - 649 °F | Stock |
PolyOne Edgetek® LCP-30GF/000 Liquid Crystal Polymer - 30% Glass Fiber
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 316 - 329 °C | 600 - 625 °F | Molding |
PolyOne Therma-Tech™ SF-6000 TC Polyphenylene Sulfide (PPS)
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Melt Temperature | 316 - 338 °C | 600 - 640 °F | |
LTL Color Compounds ColorFast® PCGF130 Polycarbonate, 30% Glass-Filled 30% glass-filled grade polycarbonateAll information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Mitsubishi Iupilon® E2000R 5 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 316 - 371 °C | 601 - 700 °F | |
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU) Udel® polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel® P-3500 LCD MB series polymers are particularly well suited for the fabrication of.. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Star Plastics PCGF10 Molding Grade PC with 10% Glass Information provided by Star Plastics, Inc. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Samyang Trirex® PC-3027U 6 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 316 - 321 °C | 601 - 610 °F | |
LNP Lubricomp® OCL-4036 Polyphenylene Sulfide, Carbon Fiber Reinforcement, PTFE Lubricant
(discontinued **)&l Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Melt Temperature | 316 - 321 °C | 601 - 610 °F | |
LNP Thermocomp® OF-1008 Polyphenylene Sulfide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Melt Temperature | 316 - 321 °C | 601 - 610 °F | |
LNP Lubricomp® PDX-O-97635 Polyphenylene Sulfide, Carbon Fiber Reinforced, PTFE Lubricant
(discontinued **)&l Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | Molding |
PolyOne Edgetek® AM 33 GF/000 L HS Black Polyphthalamide (PPA), Glass Filled
(discontinued **) Description/Features:Heat StabilizedBlackEnhanced LubricationGlass Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | Molding |
PolyOne Edgetek® AM-20CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | Molding |
PolyOne Edgetek® AM-30CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 316 - 329 °C | 601 - 624 °F | |
LNP Lubricomp® BGU- Polyphthalamide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: Heat Stabilized, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP gr.. |
|||
Melt Temperature | 316 - 329 °C | 601 - 624 °F | |
LNP Verton™ UF-700-10 Polyphthalamide, Long Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |