Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 293 - 310 °C | 559 - 590 °F | |
PolyOne OnForce™ LFT NN-30 LGF/000 Natural Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Melt Temperature | 293 - 310 °C | 560 - 590 °F | |
PlastiComp Complet® LCF50 - PA66 Nylon 66, 50% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Melt Temperature | 293 - 310 °C | 560 - 590 °F | |
PlastiComp Complet® LGF40 - PA66 MT Nylon 66, 40% Long Glass Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% long glass fiber reinforcementImpact modifiedInformation provided by.. |
|||
Melt Temperature | 293 - 310 °C | 560 - 590 °F | |
PlastiComp Complet® LGF50 - PA66 MT Nylon 66, 50% Long Glass Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% long glass fiber reinforcementImpact modifiedInformation provided by .. |
|||
Melt Temperature | 293 - 316 °C | 560 - 600 °F | |
Polymer Resources PPX-MF-FRG20 Modified-PPO, 40% Glass/Mineral Reinforced, Flame Retardant Modified-Polyphenylene Oxide, 40% Glass/Mineral Reinforced, Flame RetardantFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanica.. |
|||
Melt Temperature | 293 - 310 °C | 560 - 590 °F | |
PlastiComp Complet® LCF30 - PA66 Nylon 66, 30% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Melt Temperature | 293 - 316 °C | 560 - 600 °F | |
LTL Color Compounds ColorFast® PC100 Polycarbonate 10 melt standard injection molding gradeAll information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 293 - 310 °C | 560 - 590 °F | |
PlastiComp Complet® LCF50 - PA66 MT Nylon 66, 50% Long Carbon Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% carbon fiber reinforcementImpact modifiedInformation provided by Pla.. |
|||
Melt Temperature | 293 - 310 °C | 560 - 590 °F | |
PlastiComp Complet® LGF20 - PA66 Nylon 66, 20% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Melt Temperature | 293 - 316 °C | 559 - 601 °F | Stock |
PolyOne Stat-Tech™ MP-25NCF/000 Modified PPO - 25% Nickel Coated Graphite Fiber
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 293 - 316 °C | 560 - 600 °F | |
Polymer Resources PPX-G30 Modified PPO, 30% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 293 - 316 °C | 560 - 600 °F | |
Polymer Resources PPX-GP6 Modified PPO, General Purpose with HDT of 290 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 293 - 316 °C | 560 - 600 °F | |
LTL Color Compounds ColorFast® FRPC300 Polycarbonate, Flame-Retarded V2-rated polycarbonateAll information provided by LTL Color Compounders, Inc. |