Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 279 - 302 °C | 535 - 575 °F | |
Polymer Resources PPX/NY G10 PPO/Nylon 66 Alloy , 10% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Melt Temperature | 279 - 302 °C | 535 - 575 °F | |
Polymer Resources PPX/NY G20 PPO/Nylon 66 Alloy , 20% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
Polymer Resources PPX/NY G30 PPO/Nylon 66 Alloy , 30% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Melt Temperature | 279 - 302 °C | 535 - 575 °F | |
Polymer Resources PPX/NY GP2 PPO/Nylon 66 Alloy, Medium Heat Polyphenylene Oxide/Nylon 66 Alloy , General Purpose, Medium HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Melt Temperature | 279 - 302 °C | 535 - 575 °F | |
Polymer Resources PPX/NY G20 Modified PPO, 20% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
LTL Color Compounds ColorFast® NY2GF130 Nylon 66, 13% Glass-Filled 13% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
LTL Color Compounds ColorFast® NY2GF131 Nylon 66, 13% Glass-Filled, Impact Modified 13% glass-filled impact modified nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
LTL Color Compounds ColorFast® NY2GF330 Nylon 66, 33% Glass-Filled 33% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 279 °C | 534 °F | |
Chem Polymer Chemlon 109-18 G Nylon 66, 18% Glass Fiber Reinforced A highly toughened 18% glass fiber reinforced nylon 66 developed for applications requiring stiffness, creep resistance and impact resistance.Data provided by the manufacturer, Chem Polymer. |
|||
Melt Temperature | 279 °C | 534 °F | |
Chem Polymer Chemlon 109-33 G Nylon 66, 33% Glass Fiber Reinforced A highly toughened 33% glass fiber reinforced nylon 66 developed for applications requiring stiffness, creep resistance and impact resistance.Data provided by the manufacturer, Chem Polymer. |
|||
Melt Temperature | 279 °C | 534 °F | |
Chem Polymer Chemlon 113 G Nylon 66, 13% Glass Fiber Reinforced A 13% glass fiber reinforced nylon 66 offering improved creep resistance, stiffness, tensile strength and dimensional stability over unmodified nylon 66 materials.Data provided by the manufacturer, .. |
|||
Melt Temperature | 279 °C | 534 °F | |
Chem Polymer Chemlon 115 G Nylon 66, 15% Glass Fiber Reinforced A 15% glass fiber reinforced nylon 66 offering improved creep resistance, stiffness, tensile strength and dimensional stability over unmodified nylon 66 materials. This product offers slight improv.. |
|||
Melt Temperature | 279 °C | 534 °F | |
Chem Polymer Chemlon 104-13 G Nylon 66, 13% Glass Fiber Reinforced A toughened, 13% glass fiber reinforced nylon 66 exhibiting improved toughness and ductility, especially dry as molded.Data provided by the manufacturer, Chem Polymer. |
|||
Melt Temperature | 279 - 302 °C | 535 - 575 °F | |
Polymer Resources PPX/NY G10 Modified PPO, 10% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
Polymer Resources PPX/NY G30 Modified PPO, 30% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 279 - 302 °C | 535 - 575 °F | |
Polymer Resources PPX/NY GP2 Modified PPO, Medium Heat PPX/Nylon 6,6 Alloy
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
LTL Color Compounds ColorFast® NY1 Nylon 6 Injection molding nylon 6, with or without lubeAll information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
LTL Color Compounds ColorFast® NY1GF130 Nylon 6, 13% Glass-Filled 13% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
LTL Color Compounds ColorFast® NY1GF330 Nylon 6, 33% Glass-Filled 33% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
LTL Color Compounds ColorFast® NY2 Nylon 66 Nylon 6,6 with or without lubeAll information provided by LTL Color Compounders, Inc. |