Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 271 - 288 °C | 520 - 550 °F | |
PlastiComp Complet® LGF60 - PA6 Nylon 6, 60% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 60% long glass reinforcementInformation provided by PlastiComp, Inc. |
|||
Melt Temperature | 271 - 299 °C | 520 - 570 °F | |
Polymer Resources PC/ABS-G10 General Purpose PC/ABS Alloy, 10% Glass Filled PC/ABS Alloy, General Purpose, 10% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi.. |
|||
Melt Temperature | 271 - 288 °C | 520 - 550 °F | |
Ravago Manufacturing Americas Hylex® P1318LLT Polycarbonate Information provided by Ravago. |
|||
Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
PTS Trimid® N66-100L Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
PTS Trimid® N66-1010L Lubed, Utility Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
PTS Trimid® N66-G13 13% Glass Fiber Reinforced Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
PTS Trimid® N66-G33 33% Glass Fiber Reinforced Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
PTS Trimid® N66-T100 Toughened Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 271 - 299 °C | 520 - 570 °F | |
PTS Tristar® PC-05GFR 5% Glass Reinforced Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 271 - 293 °C | 520 - 559 °F | |
PolyOne Edgetek® NY-20GF/10GB/000 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Melt Temperature | 271 - 299 °C | 520 - 570 °F | |
Polymer Resources PC/ABS-G30 General Purpose PC/ABS Alloy, 30% Glass Filled PC/ABS Alloy, General Purpose, 30% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi.. |
|||
Melt Temperature | 271 - 304 °C | 520 - 580 °F | |
Polymer Resources PPX-SF2 Modified PPO, Structural Foam Grade, Standard Flow
(Unverified Data**) Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
Ravago Manufacturing Americas Hylon® N1000NL2 Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Melt Temperature | 271 - 288 °C | 520 - 550 °F | |
Ravago Manufacturing Americas Hylon® N1025HLFR Nylon 6/6, 25% Fiberglass, Heat Stabilized, Lubricated, Flame retardant (Cond) Information provided by Ravago. |
|||
Melt Temperature | 271 - 288 °C | 520 - 550 °F | |
Ravago Manufacturing Americas Hylon® N1025HLFR Nylon 6/6, 25% Fiberglass, Heat Stabilized, Lubricated, Flame retardant (DAM) Information provided by Ravago. |
|||
Melt Temperature | 271 - 282 °C | 520 - 540 °F | |
Firestone CG430-001 Nylon 6, 30% Fiberglass Filled Natural color. Heat stabilized. Fiber size is 4 mm length and 14 µm diameter.Information provided by Firestone |
|||
Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
MRC Polymers NAXELLâ„¢ PC110-919 General Purpose Polycarbonate, Medium High MFR Polycarbonate for colorable productsMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedCan be clear to color matchedNot for products that req.. |
|||
Melt Temperature | 271 - 304 °C | 520 - 580 °F | |
Wellman Wellamid® XT1482-BK High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
Clariant Renol 66G15BL-195 Blue Nylon 66, 15% Glass Fiber Reinforced Data provided by Clariant Masterbatches |
|||
Melt Temperature | 271 - 299 °C | 520 - 570 °F | |
Clariant Renol PA111G50 Nylon 66, 50% Glass Fiber Data provided by Clariant Masterbatches |
|||
Melt Temperature | 271 - 293 °C | 520 - 560 °F | |
Clariant Renol PA121 Nylon 66, Impact Modified Data provided by Clariant Masterbatches |
|||
Melt Temperature | 271 °C | 520 °F | |
Chem Polymer Chemlon 100 W Nylon 66, MoS2 Filled A molybdenum disulfide modified nylon 66 exhibiting superior tensile strength and wear resistance, greater dimensional stability and higher heat resistance than general purpose nylon 66.Data provide.. |
|||
Melt Temperature | 271 °C | 520 °F | |
Chem Polymer Chemlon 100 Nylon 66, Lubricated GP A medium viscosity, general purpose injection molding grade nylon 66. Internally lubricated for excellent feed and mold release properties.Data provided by the manufacturer, Chem Polymer. |
|||
Melt Temperature | 271 - 293 °C | 520 - 559 °F | Stock |
PolyOne Edgetek® NI-30CF/000 Nylon 6/10 - 30% Carbon Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 271 - 288 °C | 520 - 550 °F | Stock |
PolyOne Edgetek® NI-30GF/000 Nylon 6/10 - 30% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 271 - 410 °C | 520 - 770 °F | Average value: 352 °C Grade Count:9 |
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc.. |