Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 265 - 300 °C | 509 - 572 °F | |
SABIC 6318B Linear Low Density Polyethylene for Cast Film Product Description: 6318B is a hexene copolymer Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high process.. |
|||
Melt Temperature | 265 - 280 °C | 509 - 536 °F | Do not melt above 280°C |
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr.. |
|||
Melt Temperature | 265 - 280 °C | 509 - 536 °F | ISO 294 |
Gromax BFG30-FU03B3 Nylon 6 32.9% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 265 - 275 °C | 509 - 527 °F | |
Lavergne VYTEEN PC/ABS 8515 Polycarbonate - Acrylonitrile Butadiene Styrene Alloy Vyteen PC/ABS 8515 is an enhanced PC/ABS alloy with balanced impact/stiffness properties designed for injection molding applications.Features: -High resilience -Excellent processability -High def.. |
|||
Melt Temperature | 265 - 275 °C | 509 - 527 °F | |
Lavergne VYTEEN PC/ABS 8515XF Polycarbonate - Acrylonitrile Butadiene Styrene Alloy Vyteen PC/ABS 8515XF is an enhanced PC/ABS alloy with balanced impact/stiffness properties designed for injection molding applications.Features: -High resilience -Excellent processability -High d.. |
|||
Melt Temperature | 265 - 300 °C | 509 - 572 °F | |
LATI Latilub 87/24UV-20T PC, PTFE Filled Self-lubricating product based on Polycarbonate (PC). UV stabilized. PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri.. |
|||
Melt Temperature | 265 °C | 509 °F | Injection molding |
Styrolution Terblend® N NG-06 30% Glass Filled ABS/PA6 (Dry) Terblend N NG-06 is a 30% glass fiber reinforced ABS/PA6 blend with extra high rigidity and dimensional stability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.. |
|||
Melt Temperature | 265 °C | 509 °F | Injection molding |
Styrolution Terblend® N NM-12 ABS/PA6 (Conditioned) Terblend N NM-12 is an ABS/PA6 blend combining high impact strength and rigidity with an excellent processability and surface appearance.Information provided by STYROLUTION, which is a joint venture.. |
|||
Melt Temperature | 265 °C | 509 °F | |
Samyang Tribit® 1500GN30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A.. |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 GV 15 HWCP 15% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 GV 20 HWCP 20% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 GV 25 DCHP 25% Glass Fiber Nylon 66, Special Heat Ageing Stabilization, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 GV 25 HWCP 25% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 GV 25 HWCP 25% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 GV 30 HW 30% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 GV 30 HWCP 30% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 GV 35 HWCP 35% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 GV 40 HWCP 40% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 GV 45 HWCP 45% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 MF30 HWCP 30% Milled Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 MR 309 HWCP 30% Mineral Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600/50 GV 15 HWCP 15% Glass Fiber Nylon 66, Impact Modified Until 0°C, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600/58 GV 30 HWCP 30% Glass Fiber Nylon 66, Impact Modified Until -40°C, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 275 °C | 509 - 527 °F | |
Eurostar Staramide AST03 PA66, Impact Modified, Injection Molded AST03 is an Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Melt Temperature | 265 - 280 °C | 509 - 536 °F | |
Eurostar Starflam RFB247EX PA66/6, Glass Bead/Fiber Filled, Flame Retardant, Injection Molded RFB247EX is a Halogen Free and Red Phosphorous Free Flame Retardant, Glass Bead/ Glass Fiber Reinforced Polyamide 66/ Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 265 - 290 °C | 509 - 554 °F | |
CP-Polymer-Technik Wellamid® 6600 GS 20 HWCP 20% Glass Sphere Filled Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |