Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 257 °C | 495 °F | |
Ravago Manufacturing Americas Hylac® PL75 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Melt Temperature | 257 - 277 °C | 495 - 531 °F | Injection |
Covestro Petlon® 4630 Semi-Crystalline PET, 30% Glass Fiber
(discontinued **) Characteristics: Flame Retardant: Electrical Properties, High Heat and Chemical ResistanceApplications: Connectors, Relays, Switches, Automotive (Under Hood), AppliancesProcessing: Injection Molding.. |
|||
Melt Temperature | 257 - 277 °C | 495 - 531 °F | Injection |
Covestro Petlon® 7530 Semi-Crystalline PET, 35% Mineral/Glass Fiber
(discontinued **) Characteristics: Excellent Electrical Properties, High Heat and Chemical ResistanceApplications: Automotive (Under Hood), Appliances, Casings and HousingsProcessing: Injection Molding (Melt Temperat.. |
|||
Melt Temperature | 257 - 277 °C | 495 - 531 °F | Injection |
Covestro Petlon® 8535 Semi-Crystalline PET, 35% Mineral/Glass Fiber
(discontinued **) Characteristics: Impact Modified: Excellent Electrical Properties, High Heat ResistanceApplications: Automotive (Under Hood), Appliances, Casings and HousingsProcessing: Injection Molding (Melt Temp.. |
|||
Melt Temperature | 257 - 277 °C | 495 - 531 °F | Injection |
Covestro Petlon® DP3-1018 Semi-Crystalline PET, 35% Mineral/Glass Fiber
(discontinued **) Characteristics: Flame Retardant: Good Processability, Low Warpage, High RigidityApplications: Appliance, Telecommunication and Electrical HousingsProcessing: Injection Molding (Melt Temperature: 49.. |
|||
Melt Temperature | 257 - 277 °C | 495 - 531 °F | Injection |
Covestro Petlon® DP3-1027 Semi-Crystalline PET, 45% Glass Fiber
(discontinued **) Characteristics: General Purpose: Good Strength, High Rigidity and Heat ResistanceApplications: Automotive Valve Covers, Pump Components and PulleysProcessing: Injection Molding (Melt Temperature: 4.. |
|||
Melt Temperature | 257 - 277 °C | 495 - 531 °F | Injection |
Covestro Petlon® DP3-1039 Semi-Crystalline PET, 35% Glass Fiber
(discontinued **) Characteristics: Impact Modified: Good Strength and ToughnessApplications: Automotive Valve Covers, Pump Components and PulleysProcessing: Injection Molding (Melt Temperature: 495-530°F, Mold Tempe.. |
|||
Melt Temperature | 257 - 277 °C | 495 - 531 °F | Injection |
Covestro Petlon® DP3-1042 Semi-Crystalline PET, 40% Mineral/Glass Fiber
(discontinued **) Characteristics: General Purpose: Good Strength and Dimensional Stability, Low WarpageApplications: Automotive Valve Covers, Pump Components and PulleysProcessing: Injection Molding (Melt Temperatur.. |
|||
Melt Temperature | 257 - 277 °C | 495 - 531 °F | Injection |
Covestro Petlon® 4835 Semi-Crystalline PET, 35% Mineral/Glass Fiber
(discontinued **) Characteristics: Flame Retardant: Good Processability, Low Warpage, High RigidityApplications: Appliance, Telecommunication and Electrical HousingsProcessing: Injection Molding (Melt Temperature: 49.. |
|||
Melt Temperature | 257 °C | 495 °F | |
Teknor Apex Chemlon® 104-13 GH Nylon 66, 13% Glass Fiber Reinforced Notes: Impact Modified; Reinforced with 13% Glass Fibers; Synergistic compound exhibiting impact strength and dimensional stability Features: Good Dimensional stability; Good Processability; Heat St.. |
|||
Melt Temperature | 257 °C | 495 °F | |
Teknor Apex Chemlon® 113 GH Nylon 66, 13% Short Glass Fiber Reinforced Features: Good creep Resistance; Good stiffness; Good dimensional stability; High strength; Heat stabilized Processing Method: Injection Molding Forms: Pellets Automotive Specifications: Chrysler MS.. |
|||
Melt Temperature | 257 °C | 495 °F | |
Teknor Apex Chemlon® 140 MH Nylon 66, 40% Mineral Reinforced Notes: 40% Mineral; High rigidity with exceptional control of warpage and surface sink marks; Excellent for large parts; Fast cycling Features: Fast Molding Cycle; High Rigidity; Heat Stabilized; Lo.. |
|||
Melt Temperature | 257 - 277 °C | 495 - 531 °F | Injection |
Covestro Petlon® 3530 Semi-Crystalline PET, 30% Glass Fiber
(discontinued **) Characteristics: Excellent Electrical Properties, High Heat and Chemical ResistanceApplications: Automotive (Underhood), Appliances, Casings and HousingsProcessing: Injection Molding (Melt Temperatu.. |