Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 250 - 280 °C | 482 - 536 °F | |
Plastcom SLOVAMID 6 GF 35 Polyamide 6, 35% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 35% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Plastcom SLOVAMID 6 GF 5 T 20 FRG 2 PA6, 5% glass fibre, 20% mineral filling FeaturesPA 6 for injection moulding, with halogen free flame retardant based on polyphosphate. Good anisotrophi shinking. Application for the electrical industry: protectors, coil forms, covers, ter.. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Plastcom SLOVAMID 6 BT LS Polyamide 6, UV Stabilized FeaturesPA 6 for injection moulding with the content of UV stabilizer predetermines products for external use, eg. seats for sport stadiums, covers of electrical appliances. Delivered in natural an.. |
|||
Melt Temperature | <= 250 °C | <= 482 °F | |
EVALCA EVAL® LC-E151B Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming, solid phase pressure forming, blow molding, tubes EVOH is used in packaging applications because of its outstanding gas.. |
|||
Melt Temperature | 250 - 280 °C | 482 - 536 °F | Start Point: 260°C |
Kingfa JH820 Modified PC Features:Excellent balance propertiesSuper high impact strengthHigh stiffnessGood size stabilityGood surface, high glossHigh transparencyApplications:Injection moldingHousehold applianceBusiness mac.. |
|||
Melt Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
LG Chemical LUMID GP2130A(W) PA6+GF13%, General Purpose Feature: Injection Molding, PA6+GF13%, General PurposeApplication: Automotive PartsCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | Injection Molding |
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®.. |
|||
Melt Temperature | <= 250 °C | <= 482 °F | |
Supreme Petrochem SP 556 Flame Retardant Polystyrene Characteristics Good flow properties Good balance of toughness and rigidity Available in any color Processing Extrusion MoldingApplications T.V. Cabinets, computer monitor, printer housing Elect.. |
|||
Melt Temperature | 250 - 260 °C | 482 - 500 °F | |
A. Schulman SCHULADUR® A GF15 15% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Melt Temperature | 250 - 260 °C | 482 - 500 °F | |
A. Schulman COMTUF® 420 Impact Modified PBT Information provided by A. Schulman. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Eastman Eastar DN001HF Copolyester Applications:DisplaysPersonal care and CosmeticsProduct Description: Eastar Copolyester DN001HF has excellent flow characteristics while maintaining superior mechanical properties. It is easy to p.. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Covestro Makroblend® KU 2-7608 Polycarbonate + PBT, Mineral Filled Impact Grade ISO 7792-1-PC/PBT,MHPR,-030,MD10(PC+PBT)-blendsimpact modifiedInjection molding grade 10% mineral filledPreprocessingMax. Water content |
|||
Melt Temperature | 250 - 280 °C | 482 - 536 °F | |
CP-Polymer-Technik Wellamid® 6000 GVZ 30 HWCP 30% Glass Fiber Z-Qualities Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 250 - 280 °C | 482 - 536 °F | |
CP-Polymer-Technik Wellamid® 6000/52 GV 15 HWCP 15% Glass Fiber Nylon 6, Low Temperature Impact Modified, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 250 - 280 °C | 482 - 536 °F | DAM; Injection Molding |
DuPont Performance Polymers Zytel® FN727 BK230A Nylon 6 Zytel® FN727 BK230A is a black, impact modified, plasticizer free, very flexible polyamide 6 alloy resin having good low temperature toughness, good heat aging and good chemical resistance. Uses in.. |
|||
Melt Temperature | 250 - 260 °C | 482 - 500 °F | |
Eurostar Staramide B28H PA6, Heat Stabilized, Injection Molded Staramide B28H is a Heat Stabilized, Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 250 - 260 °C | 482 - 500 °F | |
Eurostar Staramide PX06093 PA6, Impact Modified, Injection Molded Staramide PX06093 is an UV Stabilized, Impact Modified Polyamide 6 Injection Molding Resin (also known as P1000HI020UVL)Information provided by Eurostar. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Eurostar Starflam PK0022E PA6, 10% Mineral Filled, Injection Molded PK0022E is a Halogen Free and Phosphorous Free, Mineral Filed, Polyamide 6 Injection Molding (also known as PM3620Z22 or PA 10E6 U9 Z22)Information provided by Polymer Technology & Services, the Nor.. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Eurostar Starflam PX05003 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX05003 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 250 - 265 °C | 482 - 509 °F | |
Ecomass® 705BI79 BaSO4 Filled ABS Nontoxic alternative to traditional materials, radiation shielding applications.Moderate Specific GravityBaSO4 Powder Filled ABSInformation provided by Technical Polymers |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Covestro Makroblend® KU 2-7912/4 Polycarbonate + PBT, Impact Grade ISO 7792-1-PBT/PC,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessingMax. Water content |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Eurostar Starflam BFR330A PA6, Glass Bead Reinforced, Flame Retardant, Injection Molded Starflam BFR330A is a Flame Retardant, Glass Bead Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Eurostar Starflam PK0052E PA6, 25% Mineral Filled, Injection Molded PK0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Mineral Filed, Polyamide 6 Injection Molding (also known as PM3520Z222 or PA 25E6 U9 Z22)Information provided by Polymer Technolo.. |
|||
Melt Temperature | 250 - 290 °C | 482 - 554 °F | Injection-molding/Extrusion |
BASF Ultramid® B3WGM 24 HP BK 23210 10/20% Glass/Mineral Filled PA6-1 (Conditioned) Description: 20% mineral-filled and 10% glass-fiber reinforced injection-molding grade with outstanding flowability for technical parts with medium rigidity and high dimensional stability, e.g. for.. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection-molding/Extrusion |
BASF Ultramid® FRee B3U31G4 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | Injection-molding/Extrusion |
BASF Ultramid® B3S HP PA6 (Conditioned) Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing |
|||
Melt Temperature | 250 °C | 482 °F | Injection Molding |
Ineos ABS Lustran® 452
(discontinued **) Key Features:UnfilledSuitable processing methods:Sheet extrusionThermoformingInformation provided by Bayer Polymers.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after I.. |
|||
Melt Temperature | <= 250 °C | <= 482 °F | |
Supreme Petrochem SP201 4551 Light Stabilized Polystyrene Characteristics Excellent light stability to fluorescent & incandescent light sources Very high clarity and heat resistance Excellent strength & stiffness Processing Injection molding Extrusion A.. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection molding/Extrusion |
BASF Ultradur® B 4300 G6 HR 30% Glass Filled BK 15116 PBT Description: injection-molding grade with 30% glass-fibers; for rigid and dimensionally stable technical parts with increased requirements on hydrolysis resistance. For example automotive connectors.. |