Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 245 °C | 473 °F | Optimum; Injection Molding |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET
(Unverified Data**) Hytrel® DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 49D and contains fine particle size carbon black.In.. |
|||
Melt Temperature | 245 °C | 473 °F | Optimum; Injection Molding |
DuPont Performance Polymers Hytrel® 7246HS BK320 TPC-ET
(Unverified Data**) Hytrel® 7246HS BK320 is a high modulus, heat stabilized, black grade with nominal hardness of 72D.Information provided by DuPont |
|||
Melt Temperature | 245 - 265 °C | 473 - 509 °F | Start Point: 255°C |
Kingfa PA66-ROW Halogen-free, Flame Retardant PA66 Features:Flame retardantHigh mechanical strengthHigh heat resistanceGood electric propertiesNo bloomingApplications:Injection moldingConnectors, linkersRelay, bobbins, plugsHousehold appliance parts.. |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2156FL PBT+GF15% Description: Injection Molding, PBT+GF15%, Flame Retardant Application: IT/OA, E&E (CRT Socket)CAS No. 68928-70-1, 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by.. |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2200 PBT+GF20% Description: Injection Molding, PBT+GF20%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2300R PBT+GF30% Description: Injection Molding, PBT+GF30%, Anti-HydrolysisApplication: E&E (Speed Nut & Body)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2306FI PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant, High Impact Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical.. |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® HI2152 PBT+GF15% Description: Injection Molding, PBT+GF15%, High ImpactApplication: IT/OA, E&E (Bobbin, Switch)CAS No. 9003-01-04, 65997-17-3, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® SG3250 PBT+PET+MF25% Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® SG3250A PBT+PET+MF25% Description: Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Melt Temperature | 245 - 265 °C | 473 - 509 °F | Injection Molding |
Ineos ABS Lustran® 288 ABS, Injection Molding Grade Lustran® ABS 288 is a very high-flow injection molding grade of ABS (acrylonitrile butadiene styrene) with good impact strength and high gloss. It is intended for use in a wide range of applicati.. |
|||
Melt Temperature | 245 - 270 °C | 473 - 518 °F | Injection Molding |
LG Chemical LUPOY SG5009FA PC/ABS/PMMA, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High Gloss, Anti-scratchApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9, 9011-14-7 and 181028-79-5Informatio.. |
|||
Melt Temperature | 245 °C | 473 °F | LCL-PR29 |
Intercontinental Polymers 188 PET Polymer Type - Clear, Alkali Soluble, Polyester Pellets Applications: Filament SpecialtiesInformation provided by Intercontinental Polymers. |
|||
Melt Temperature | 245 - 260 °C | 473 - 500 °F | ISO 294 |
Gromax BTQ50-EQ00N1 Nylon 6, Impact Modified (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2156FM PBT+GF15% Description: Injection Molding, PBT+GF15%, Flame Retardant Application: IT/OA, E&E (CRT Socket)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Melt Temperature | 245 - 260 °C | 473 - 500 °F | ISO 294 |
Gromax BTE70-FN001N1 Nylon 6 (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 245 - 260 °C | 473 - 500 °F | ISO 294 |
Gromax BTQ50-DQ00N1 Nylon 6, Impact Modified (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 245 - 260 °C | 473 - 500 °F | ISO 294 |
Gromax BTQ50-EQ00N1 Nylon 6, Impact Modified (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 245 °C | 473 °F | |
Samyang Tribit® 1503S Polybutylene Terephthalate Characteristics:High impactApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provided by Samyang |
|||
Melt Temperature | 245 - 265 °C | 473 - 509 °F | |
CP-Polymer-Technik Wellamid® 6000 S Nylon 6, Finely Crystalline, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 245 - 265 °C | 473 - 509 °F | |
CP-Polymer-Technik Wellamid® 6000 SUVCP Nylon 6, Finely Crystalline, UV Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 245 - 260 °C | 473 - 500 °F | |
CP-Polymer-Technik Wellamid® 6000/42 Nylon 6, Polymer Modified, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 245 - 260 °C | 473 - 500 °F | |
CP-Polymer-Technik Wellamid® 6000/50 CP Nylon 6, Impact Modified Until 0°C, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 245 - 260 °C | 473 - 500 °F | |
CP-Polymer-Technik Wellamid® 6000/50 HWUVCP Nylon 6, Impact Modified Until 0°C, UV Stabilized, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 245 - 260 °C | 473 - 500 °F | |
CP-Polymer-Technik Wellamid® 6000/58 CP Nylon 6, Impact Modified Until -40°C, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 245 °C | 473 °F | Optimum; Blow Molding |
DuPont Performance Polymers Hytrel® BM6574 BK316 TPC-ET
(Unverified Data**) Hytrel® BM6574 is a 65 nom. Shore D, plasticiser free high performance resin for blow molding and extrusion; it shows ageing resistance up to 150°C, and excellent mechanical properties at elevated.. |
|||
Melt Temperature | 245 °C | 473 °F | Optimum; Injection Molding |
DuPont Performance Polymers Hytrel® DYM1300 BK320 TPC-ET
(Unverified Data**) Hytrel® DYM1300 is a high performance thermoplastic elastomer with high modulus, suited for air bag door applications.Information provided by DuPont Performance Polymers |
|||
Melt Temperature | 245 - 270 °C | 473 - 518 °F | Injection molding |
BASF Ultradur B 2550 PBT Ultradur B2550 is an unfilled, very free-flowing grade for coating paper and board with high heat resistance, for example for packaging of frozen goods and ready-prepared meals. Also suitable for in.. |
|||
Melt Temperature | 245 - 260 °C | 473 - 500 °F | |
BASF Ultramid® 8270 HS BK 102 PA6 (Dry) Description: Ultramid 8270 HS BK-102 is a thermally modified pigmented black, PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile ex.. |