Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 243 - 266 °C | 470 - 510 °F | Molding |
PolyOne Lubri-Tech™ PS-15GF/10T Polybutylene Terephthalate (PBT), Glass Filled, PTFE Lubricated
(discontinued Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 HB (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 243 - 277 °C | 470 - 530 °F | Molding |
PolyOne Edgetek® PS-20CF/000 Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 243 - 277 °C | 470 - 530 °F | Molding |
PolyOne Stat-Tech™ PS-NX 102902 CM Black Polybutylene Terephthalate (PBT)
(discontinued **) Preliminary Data SheetPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 243 - 310 °C | 469 - 590 °F | Average value: 284 °C Grade Count:3 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
Melt Temperature | 243 °C | 469 °F | Injection |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 5% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Melt Temperature | 243 °C | 469 °F | Injection |
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 8% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Melt Temperature | 243 - 279 °C | 470 - 535 °F | Average value: 261 °C Grade Count:11 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
Melt Temperature | 243 °C | 469 °F | Tubular (Blown) Film |
Honeywell Aegis™ HCA95ZP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA95ZP is a medium viscosity, nylon 6/6,6 film extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500. It p.. |
|||
Melt Temperature | 243 - 300 °C | 470 - 572 °F | Average value: 269 °C Grade Count:10 |
Overview of materials for Nylon 6, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria.. |