Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 220 - 230 °C | 428 - 446 °F | |
Polyplastic Armlen® PP MF 20-3IM Impact Modified Polypropylene Impact modified polypropylene composite materialInformation provided by PolyPlastic Group. |
|||
Melt Temperature | 220 - 260 °C | 428 - 500 °F | |
Premix Thermoplastics PRE-ELEC® ABS 1410 PRE-ELEC ABS 1410 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ABS 141.. |
|||
Melt Temperature | 220 - 250 °C | 428 - 482 °F | Injection Molding |
DuPont Performance Polymers Hytrel® 5553FG NC010 TPC-ET
(Unverified Data**) Hytrel® 5553FG NC010 is a high performance thermoplastic polyester elastomer with food compliance specificity.Information provided by DuPont |
|||
Melt Temperature | 220 °C | 428 °F | |
Chevron Phillips 7109T LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene CopolymerCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Industrial Liners, Stretch Wrap, Garment Bags.. |
|||
Melt Temperature | 220 °C | 428 °F | |
Chevron Phillips 7109BK Linear low density polyethylene blown film resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymer, blow film resin, medium slip, medium antiblock version of 7109Characteristics: good stiffness at thin gauges, good drawdown, low COF, c.. |
|||
Melt Temperature | 220 - 305 °C | 428 - 581 °F | Extrusion Coating |
DuPont Nucrel® 30707HS Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating
(discontinued **) 7 wt% Acrylic Acid.Nucrel® 30707HS is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusio.. |
|||
Melt Temperature | 220 - 250 °C | 428 - 482 °F | Start Point: 240°C |
Kingfa HR-528 Modified ABS Features:UL94 HB @ 1.5-3.2mmExcellent heat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd... |
|||
Melt Temperature | 220 - 250 °C | 428 - 482 °F | Start Point: 230°C |
Kingfa JH950-602 Low-temperature Resistant & Flame Retardant PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh heat resistanceGood normal/low temperature impact strengthGood surface, high glossApplications:ControllerPlug, socketShell of ammeterSmall hou.. |
|||
Melt Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LG703W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Filllar Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided.. |
|||
Melt Temperature | 220 - 250 °C | 428 - 482 °F | |
LG Chemical LI-913 ASA, Injection Molding, High Impact Information Provided by LG Chem |
|||
Melt Temperature | 220 - 250 °C | 428 - 482 °F | |
LG Chemical NS-161 ABS, Antistatic, High Strength Information Provided by LG Chem |
|||
Melt Temperature | 220 - 260 °C | 428 - 500 °F | ISO 294 |
Styrolution Terluran® GP-25 ABS Terluran GP-25 is an easy-flow, general purpose injection molding grade with high resistance to impact and heat distortion; intended for a wide range of applications, particularly in the housings se.. |
|||
Melt Temperature | <= 220 °C | <= 428 °F | |
Supreme Petrochem SC 6501 Toughened Polystyrene Characteristics Excellent melt strength Extremely tough Easy printability Easy miscibility with most grades of polystyrene Processing Extrusion Thermoforming Injection MoldingApplications Impac.. |
|||
Melt Temperature | <= 220 °C | <= 428 °F | |
Supreme Petrochem SP 256 Toughened Polystyrene Characteristics Superior flexibility Good ball drop strength Excellent clarity Easy flow Processing Injection moldingApplications Transparent hangers Stationery items like pen barrels, geometric .. |
|||
Melt Temperature | 220 - 260 °C | 428 - 500 °F | |
Sax Polymers SAXLAC 310T Acrylonitrile Butadiene Styrene Saxalac 310T is an antistatic, high impact resistant ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid.. |
|||
Melt Temperature | 220 - 260 °C | 428 - 500 °F | Polymer Mass Temp |
Borealis Daplen™ EG203AE Polypropylene Compound Elastomer and Mineral Modified Daplen EG203AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EG203AE is a material with excellent impact /stiffness ratio. Thanks to its low .. |
|||
Melt Temperature | 220 - 260 °C | 428 - 500 °F | |
Borealis HG430MO Polypropylene HG430MO is a polypropylene homopolymer intended for injection molding. This polymer product is characterized by a superior impact resistance. This grade has ductile failure in falling weight impact .. |
|||
Melt Temperature | 220 - 240 °C | 428 - 464 °F | |
Tisan TISLAMID® 6 30% Glass Filled Impact Modified Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Melt Temperature | 220 - 260 °C | 428 - 500 °F | Polymer Mass Temp |
Borealis Daplen™ EE109AE TPO Compound Daplen EE109AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE109AE is a material with excellent impact /stiffness ratio. Thanks to its low .. |
|||
Melt Temperature | 220 - 270 °C | 428 - 518 °F | |
Borealis Xmod™ GD301HP High Performance 32% Glass Fiber Reinforced Xmod GD301HP is reinforced with 32% chemically coupled glass fibers and based on specific Polymer matrix material which is bringing excellent mechanical properties (impact behavior) and very good st.. |
|||
Melt Temperature | 220 °C | 428 °F | |
E-Polymers TEKAMID® H12TW Unreinforced Low warpage PA/ABS Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB.. |
|||
Melt Temperature | 220 °C | 428 °F | |
Carmel Olefins IPETHENE® 100 Low Density Polyethylene IPETHENE® 100 is a low density polyethylene extrusion grade. It exhibits good impact and puncture resistance, good processability and good ESCR. APPLICATIONS IPETHENE® 100 is used for production.. |
|||
Melt Temperature | 220 - 225 °C | 428 - 437 °F | |
Beijing Ranger Chem BLUESTAR® 1079 PBT Can be used directly for spinning, and producing color concentrates. It can also be used for production after reinforcement & compounding.Information provided by Beijing Ranger Chemical Co. |
|||
Melt Temperature | 220 - 260 °C | 428 - 500 °F | |
Plastcom SLOVALEN PH 69 GF 30/1M Polypropylene reinforced with glass fiber Modified homopolymer PP for injection molding, reinforced with 30% glass fiber. Applied in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Pl.. |
|||
Melt Temperature | 220 - 343 °C | 428 - 650 °F | Average value: 301 °C Grade Count:60 |
Overview of materials for Polycarbonate, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Melt Temperature | 220 - 260 °C | 428 - 500 °F | Polymer Mass Temp |
Borealis Daplen™ EE103AE TPO Compound Daplen EE103AE is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE103AE is a material with excellent impact /stiffness ratio. Thanks to its low .. |
|||
Melt Temperature | 220 - 260 °C | 428 - 500 °F | Resin, Injection Molding |
LG Chemical LUTENE-H ME8000 HDPE Description: LUTENE-H ME8000 is mainly intended for injection molding of containers. It has good mechanical properties and high productivity.Applications: Silicone cartridge, containers, complicated.. |
|||
Melt Temperature | 220 - 250 °C | 428 - 482 °F | |
Sax Polymers SAXALEN PPH304G25 Polypropylene Homopolymer, 25% Glass Filled SAXALEN PPH304G25 is a 25% glass filled Polypropylene - Homopolymer intended for injection molding. This compound is characterized by high stiffness good impact resistance und reduced creep under lo.. |
|||
Melt Temperature | 220 - 250 °C | 428 - 482 °F | |
LG Chemical HG-174 ABS, High Gloss, Super High Flow Information Provided by LG Chem |