Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 210 - 230 °C | 410 - 446 °F | |
PolyOne OnForce™ LFT PP-50LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Melt Temperature | 210 - 221 °C | 410 - 430 °F | |
PlastiComp Complet® LGF20 - PP Homopolymer Polypropylene, 20% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 20% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Melt Temperature | 210 °C | 410 °F | Extrusion |
ExxonMobil Santoprene® 243-50 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Melt Temperature | 210 °C | 410 °F | Extrusion |
ExxonMobil Santoprene® 273-50 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Melt Temperature | 210 - 240 °C | 410 - 464 °F | Extrusion |
Polimeri Europa Edistir RCL 600 Polystyrene
(discontinued **) Special medium impact polystyrene extrusion grade exhibiting very high gloss. This grade should be used where is required an excellent surface finish. It can be directly extruded in foils and sheets.. |
|||
Melt Temperature | 210 - 232 °C | 410 - 450 °F | |
Ineos Nova Zyntar® F7080 Developmental Flame Retardant Polystyrene
(discontinued **) Features: General purpose non-Deca based resin (does not combine with Decabromodiphenyloxide)Good indoor UV light color stability(grey colors)UL94 V-0 @ 1.5 mm for all colors Good aesthetics for inj.. |
|||
Melt Temperature | 210 - 220 °C | 410 - 428 °F | Injection Molding |
DuPont Performance Polymers Delrin® 100P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin® 100P provides maximum toughness in the product line without modification. Delrin® 100P has improved pro.. |
|||
Melt Temperature | 210 - 220 °C | 410 - 428 °F | Injection Molding |
DuPont Performance Polymers Delrin® 127UV BK701 Acetal Homopolymer
(Unverified Data**) Delrin® 127UV BK701 is a high viscosity, UV stabilized acetal homopolymer. It has excellent impact strength, UV resistance and thermal stability. It is well suited for automotive interior applicati.. |
|||
Melt Temperature | 210 - 220 °C | 410 - 428 °F | Injection Molding |
DuPont Performance Polymers Delrin® 300CP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of processing and part performance.Information provided by DuPont Perf.. |
|||
Melt Temperature | >= 210 °C | >= 410 °F | |
LyondellBasell Plexar® PX3216 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE Plexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copolymers, s.. |
|||
Melt Temperature | 210 - 240 °C | 410 - 464 °F | Injection Molding |
LG Chemical HI153 ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Melt Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical MP211 ABS, Low Gloss, Metal Plating Feature: Injection Molding, High Flow, Metal PlatingApplication: Decorative Parts (Home Appliance Door Handle Etc)CAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
Melt Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical MP220 ABS, High Adhesion, Heat Resistance Feature: Injection Molding, High Adhesion, Metal PlatingApplication: Automobiles Radiator Grill, MoldingCAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
Melt Temperature | 210 °C | 410 °F | Recommended Extrusion |
MBA Polymers ABS 4124 Recycled acrylonitrile-butadiene-styrene copolymer Available in standard black.Information provided by MBA Polymers. |
|||
Melt Temperature | 210 - 240 °C | 410 - 464 °F | |
LG Chemical LUPOL HF-3208H High Flow Polypropylene, 20% Mineral Fillers, General Purpose LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Melt Temperature | 210 - 240 °C | 410 - 464 °F | |
LG Chemical LUPOL LW-4407 Low Warpage Polypropylene, 40% Glass Fiber/Mineral Filler Reinforced, Heat Resistant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Melt Temperature | 210 - 240 °C | 410 - 464 °F | |
LG Chemical LUPOL TE-5102 Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Impact LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Melt Temperature | 210 - 240 °C | 410 - 464 °F | |
LG Chemical LUPOL TE-5104K Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Melt Temperature | 210 - 230 °C | 410 - 446 °F | |
LATI Latilub 82-05GR G/30 PA12, 30% Glass Fiber Reinforced, Graphite Filled Self-lubricating product based on Polyamide 12 (PA12). Graphite. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Melt Temperature | 210 - 240 °C | 410 - 464 °F | |
LATI Latiohm 82-02 PD09 PA12 Semiconductive/dissipative product based on Polyamide 12 (PA12). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr.. |
|||
Melt Temperature | 210 - 230 °C | 410 - 446 °F | |
Borealis BA202E Polypropylene Block Copolymer for Non-Pressure Pipes BA202E is a high molecular weight, low melt flow rate polypropylene block copolymer with very high impact strength. Applications: BA202E is recommended for non-pressure pipes & fittings, thin-walled.. |
|||
Melt Temperature | 210 - 230 °C | 410 - 446 °F | |
Borealis BA204E Polypropylene Block Copolymer for Non-Pressure Pipes BA204E is a high molecular weight, low melt flow rate polypropylene block copolymer with very high impact strength. Applications: BA204E is recommended for non-pressure pipes & fittings, thin-walle.. |
|||
Melt Temperature | 210 - 260 °C | 410 - 500 °F | |
Borealis Borsoft™ SE410MO Polypropylene for Injection Molding Borsoft SE410MO is a specially designed modified relatively soft polypropylene heterophasic copolymer with medium melt flow intended for injection moldingBorsoft SE410MO is a tailor made grade desig.. |
|||
Melt Temperature | 210 °C | 410 °F | Cast Film |
Westlake EF528 18.5% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ EF528 is an ethylene vinyl acetate copolymer with 18.5% VA. EF528 is designed for blown and cast films requiring excellent optics and low heat seal initiation. High melt strength .. |
|||
Melt Temperature | 210 - 249 °C | 410 - 480 °F | |
Zhejiang Double Fish YS-G030 30% Long Fiber Glass Reinforced Polypropylene Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm.. |
|||
Melt Temperature | 210 - 260 °C | 410 - 500 °F | |
Borealis RG435MO Polypropylene, Transparent Random Copolymer RG435MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. Products molded from this grade exhibit excellent transparency, good gloss, high impact.. |
|||
Melt Temperature | 210 °C | 410 °F | Extrusion |
ExxonMobil Santoprene® 203-40 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Melt Temperature | 210 - 260 °C | 410 - 500 °F | |
Borealis Daplen™ ED135AI TPO Compound Daplen ED135AI is a 10% mineral filled grade intended for injection molding. ED135AI offers very good balance in stiffness/impact strengthDaplen ED135AI has been developed especially for the car in.. |
|||
Melt Temperature | 210 - 220 °C | 410 - 428 °F | Injection Molding |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG100P is a high viscosity acetal homopolymer, with improved thermal stability for use in easy to fill molds. It has been developed for consideration into applications such as parts for the.. |