Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 20.0 - 285 °C | 68.0 - 545 °F | Average value: 236 °C Grade Count:18 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Melt Temperature | 20.0 - 280 °C | 68.0 - 536 °F | Average value: 254 °C Grade Count:12 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Melt Temperature | 20.0 - 371 °C | 68.0 - 700 °F | Average value: 184 °C Grade Count:16 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Melt Temperature | 20.0 - 218 °C | 68.0 - 425 °F | Average value: 173 °C Grade Count:13 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Melt Temperature | 20.0 - 215 °C | 68.0 - 419 °F | Average value: 184 °C Grade Count:30 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
Melt Temperature | 20.0 - 220 °C | 68.0 - 428 °F | Average value: 203 °C Grade Count:10 |
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim.. |
|||
Melt Temperature | 20.0 - 399 °C | 68.0 - 750 °F | Average value: 276 °C Grade Count:11 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Melt Temperature | 20.0 - 340 °C | 68.0 - 644 °F | Average value: 292 °C Grade Count:12 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%.. |
|||
Melt Temperature | 20.0 - 345 °C | 68.0 - 653 °F | Average value: 292 °C Grade Count:19 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |
|||
Melt Temperature | 20.0 - 345 °C | 68.0 - 653 °F | Average value: 286 °C Grade Count:11 |
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |
|||
Melt Temperature | 20.0 - 277 °C | 68.0 - 531 °F | Average value: 246 °C Grade Count:16 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
Melt Temperature | 20.0 - 300 °C | 68.0 - 572 °F | Average value: 270 °C Grade Count:13 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |
|||
Melt Temperature | 20.0 - 300 °C | 68.0 - 572 °F | Average value: 262 °C Grade Count:8 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |
|||
Melt Temperature | 20.0 - 304 °C | 68.0 - 579 °F | Average value: 274 °C Grade Count:22 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |
|||
Melt Temperature | 20.0 - 270 °C | 68.0 - 518 °F | Average value: 231 °C Grade Count:15 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |