Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 171 - 179 °C | 340 - 354 °F | |
PolyOne Geon™ Vinyl Wire & Cable 1802-xx11FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable W1820L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 171 - 177 °C | 340 - 351 °F | |
PolyOne Geon™ Vinyl Wire & Cable WELB406LU Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 171 - 193 °C | 340 - 379 °F | ASTM D789 |
Niche Polymer PPHG20BK Homopolymer PP, 20% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 171 - 177 °C | 340 - 351 °F | |
PolyOne Geon™ Vinyl Flexible D75M0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 171 - 179 °C | 340 - 354 °F | |
PolyOne Geon™ Vinyl Flexible R246AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 171 - 177 °C | 340 - 351 °F | |
PolyOne Geon™ Vinyl Flexible C70T0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 171 - 177 °C | 340 - 351 °F | |
PolyOne Geon™ Vinyl Flexible C70UB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 171 - 179 °C | 340 - 354 °F | |
PolyOne Geon™ Vinyl Flexible R356AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | |
Huntsman PE1257 EVA Film Extrusion
(discontinued **) 2.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, good heat seal characteristics.Applications: Film extrusion: general purpose packaging where to.. |
|||
Melt Temperature | 171 - 220 °C | 340 - 428 °F | Average value: 190 °C Grade Count:8 |
Overview of materials for Styrene/Butadiene/Styrene (SBS) This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Butadiene/Styrene (SBS)". Each property range of values reported is minimum and maximum values o.. |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | |
Sylvin Technologies 8950-90 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | |
Sylvin Technologies 9915-90 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | |
Sylvin Technologies 9980-90 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 171 °C | 340 °F | |
Teknor Apex APEX® 3310-65 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Melt Temperature | 171 °C | 340 °F | |
Teknor Apex APEX® 90-A41R-65-NT Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by.. |
|||
Melt Temperature | 171 °C | 340 °F | |
Teknor Apex APEX® 3210-65 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Melt Temperature | 171 °C | 340 °F | |
Axiall 6704 Moldings & Extrusions Flexible PVC An expandable, low gravity, injection molding compound specifically developed for footwear applications. Finished product appearance is matte, similar to TPR.Information provided by Georgia GulfGeo.. |
|||
Melt Temperature | 171 °C | 340 °F | |
Axiall 12792 Wire & Cable Flexible PVC General purpose, 75°C rated non-lead stabilized jacket compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 171 °C | 340 °F | |
Teknor Apex APEX® 3202-65 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Caps, Closure, Connectors, Food Service Applications, Safety Equipment, Valves/Valve Parts Appearance-Cl.. |
|||
Melt Temperature | 171 °C | 340 °F | |
Axiall 8681 Moldings & Extrusions Flexible PVC General purpose, elastomeric vinyl compound well suited for co-extrusion with rigid PVC.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 171 °C | 340 °F | |
Axiall 8705 Moldings & Extrusions Flexible PVC General purpose PVC extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |