Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 157 - 207 °C | 315 - 405 °F | Average value: 182 °C Grade Count:6 |
Overview of materials for PVC/Acrylic Alloy This property data is a summary of similar materials in the MatWeb database for the category "PVC/Acrylic Alloy". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 8600-65 Clear PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 8915-65 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 8925-65 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 8940-65 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 8950-65 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 8960-65 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 8980-65 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 8999-65 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 9077-65 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 9600-65 Clear PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 9915-65 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 9925-65 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 9940-65 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 9950-65 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 9960-65 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 9980-65 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 9999-65 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |