Polymer Property : Melt Temperature = 120 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 120 - 160 °C
248 - 320 °F
Plastcom SLOVALEN EQ 71 N PP, imp. strength
FeaturesPE modified with EVA. The addition of EVA causes increased toughness. General application in all industry branches. Delivered in natural mode and in the full RAL colour scale.Packaging, tran..
Melt Temperature 120 - 238 °C
248 - 460 °F
Average value: 192 °C Grade Count:108
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim..
Melt Temperature 120 °C
248 °F
LCL-PR29
Intercontinental Polymers CoPET 159 CoPET Polymer Type - Clear, Low Melt Polyester Pellets
Applications: Low MeltInformation provided by Intercontinental Polymers.
Melt Temperature 120 - 125 °C
248 - 257 °F
Borealis FR4837 Chemically Crosslinkable Polyethylene Compound for Primary Automotive Wires
FR4837 is a chemically crosslinkable Non-halogen flame retardant Polyethylene compound for Primary Automotive and Appliance Wire. Applications: FR4837 is intended for use as a 125º C rated primary..
Melt Temperature 120 - 125 °C
248 - 257 °F
Borealis FR4847 Polyethylene Based Striping Compound
FR4847 is a Polyethylene Based Striping Compound for Primary Automotive Wires. FR4847 is designed and manufactured with advanced material and processing technology to provide enhanced stabilization..
Melt Temperature 120 - 140 °C
248 - 284 °F
Borealis LE0516 Polyethylene Compound, Crosslinkable, Semiconductive
LE0516 is a crosslinkable black polyethylene compound, specially designed for strippable semi conductive screen applications. Applications: LE0516 is intended for strippable outer semi conductive s..
Melt Temperature 120 - 140 °C
248 - 284 °F
Borealis LE0592 Polyethylene
LE0592 is a crosslinkable black polyethylene compound, specially designed for bonded semi conductive screen applications. Applications: LE0592 is intended for semi conductive applications in XLPE m..
Melt Temperature 120 - 140 °C
248 - 284 °F
Borealis Supersmooth™ LE0550 Polyethylene Insulation Compound, Crosslinkable
Supersmooth™ LE0550 is a crosslinkable black polyethylene compound, specially designed for bonded semiconductive screen applications. Applications: Supersmooth™ LE0550 is intended for semiconduct..
Melt Temperature 120 - 140 °C
248 - 284 °F
Borealis Supersmooth™ LE0592S Polyethylene
Supersmooth™ LE0592S is a crosslinkable black polyethylene compound, specially designed for bonded semiconductive screen applications. Supersmooth™ LE0592S is intended for semiconductive applicat..
Melt Temperature 120 - 230 °C
248 - 446 °F
Average value: 162 °C Grade Count:13
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an..
Melt Temperature 120 - 125 °C
248 - 257 °F
Borealis FR4832 Chemically Crosslinkable Polyethylene Compound for Primary Automotive Wires
FR4832 is a Chemically Crosslinkable Polyethylene Compound for Primary Automotive Wires. Applications: FR4832 is intended for use as a 125º C rated primary insulation for crosslinked automotive wi..
Melt Temperature 120 - 185 °C
248 - 365 °F
Borealis LE7710 Polyethylene Compound, Semiconductive, Thermoplastic
LE7710 is a thermoplastic black polyethylene compound, specially designed for semiconductive screen applications. Applications: LE7710 is intended for semiconductive applications in medium voltage ..