Polymer Property : Melt Temperature = 102 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature <= 102 °C
<= 215 °F
ExxonMobil Geolast® 701-87W183 Thermoplastic Elastomer
A hard, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic..
Melt Temperature <= 102 °C
<= 215 °F
ExxonMobil Geolast® 701-70 Thermoplastic Elastomer
A soft, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic..
Melt Temperature <= 102 °C
<= 215 °F
ExxonMobil Geolast® 701-80W183 Thermoplastic Elastomer
A soft, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic..
Melt Temperature <= 102 °C
<= 215 °F
ExxonMobil Geolast® 703-45 Thermoplastic Elastomer
A hard, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic..