Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 25 min @Temperature 25.0 °C |
25 min @Temperature 77.0 °F |
work life |
BCC Products BC 8675E Polyurethane Elastomer BC 8675E is a multi-purpose elastomer that can perform many functions. Typical product features are: easy to use, cures at room temperature, resists moisture absorption, excellent in use for molds f.. |