Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 40.0 - 60.0 min @Temperature 23.9 °C |
40.0 - 60.0 min @Temperature 75.0 °F |
when reacted at 1:1.3 by weight, based on the application |
TSE Industries EcoSPRAY® SS100 Aliphatic Polyurethane Resin TSE-EcoSPRAY® SS100 is an “Environmentally-Preferred Product” or EPP. It is an Aliphatic polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during application. TSE-EcoSPRA.. |
|||
Gel Time | 40.0 - 60.0 min @Temperature 23.9 °C |
40.0 - 60.0 min @Temperature 75.0 °F |
when reacted at 1:1.3 by weight, based on the application |
TSE Industries EzNATE® SS100 Aliphatic Polyurethane Resin TSE-EcoSPRAY® SS100 is an “Environmentally-Preferred Product” or EPP. It is an Aliphatic polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during application. TSE-EcoSPRA.. |
|||
Gel Time | 40.0 - 50.0 min @Temperature 25.0 °C |
40.0 - 50.0 min @Temperature 77.0 °F |
100 gram mass |
Lord Adhesives Thermosetâ„¢ UR-340 Two Component Urethane Encapsulant Lord UR-340 is a two component, room temperature curing, urethane encapsulating compound. It is low in viscosity and has excellent flow characteristics. Its flexibility, low modulus characteristics,.. |
|||
Gel Time | 40.0 - 60.0 min @Temperature 23.9 °C |
40.0 - 60.0 min @Temperature 75.0 °F |
when reacted at 1:1.3 by weight, based on the application |
TSE Industries EcoSPRAY® SS100 Aliphatic Polyurethane Resin TSE-EcoSPRAY® SS100 is an “Environmentally-Preferred Product” or EPP. It is an Aliphatic polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during application. TSE-EcoSPRA.. |
|||
Gel Time | 40.0 - 60.0 min @Temperature 23.9 °C |
40.0 - 60.0 min @Temperature 75.0 °F |
when reacted at 1:1.3 by weight, based on the application |
TSE Industries EzNATE® SS100 Aliphatic Polyurethane Resin TSE-EcoSPRAY® SS100 is an “Environmentally-Preferred Product” or EPP. It is an Aliphatic polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during application. TSE-EcoSPRA.. |