Processing Properties | Metric | English | Comments |
---|---|---|---|
Clamp Pressure | 27.6 - 68.9 MPa | 4000 - 10000 psi | |
PTS Tristar® PC-10R-(V6) 6 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Clamp Pressure | 27.6 - 68.9 MPa | 4000 - 10000 psi | |
PTS Tristar® PC-10R-(VE) 12 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
ExxonMobil Santoprene® 221-73 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
ExxonMobil Santoprene® 241-80 Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
ExxonMobil Santoprene® 243-50 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
ExxonMobil Vyram™ 9101-75 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
ExxonMobil Vyram™ 9103-45 Thermoplastic Elastomer
(discontinued **) A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
ExxonMobil Vyram™ 9201-85 Thermoplastic Elastomer
(discontinued **) A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
ExxonMobil Vyram™ 9203-54 Thermoplastic Elastomer
(discontinued **) A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Clamp Pressure | 27.6 - 68.9 MPa | 4000 - 10000 psi | |
PTS Tristar® PC-10FR-(18) 18 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Clamp Pressure | 27.6 - 68.9 MPa | 4000 - 10000 psi | |
PTS Tristar® PC-10FR-(V) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Clamp Pressure | 27.6 - 68.9 MPa | 4000 - 10000 psi | |
PTS Tristar® PC-10R-CL(22) 22 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Clamp Pressure | 27.6 - 68.9 MPa | 4000 - 10000 psi | |
Mitsubishi Iupilon® H2000UR 23 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Clamp Pressure | 27.6 - 68.9 MPa | 4000 - 10000 psi | |
Mitsubishi Iupilon® H3000UR 30 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Clamp Pressure | 27.6 - 68.9 MPa | 4000 - 10000 psi | |
Samyang Trirex® PC-3022U 15 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
ExxonMobil Santoprene® 103-40 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
ExxonMobil Santoprene® 121-87 Thermoplastic Elastomer A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
ExxonMobil Santoprene® 201-55 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
ExxonMobil Santoprene® 203-40 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
ExxonMobil Santoprene® 251-80W232 Thermoplastic Elastomer A soft, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retard.. |
|||
Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
ExxonMobil Santoprene® 251-92W232 Thermoplastic Elastomer A hard, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retard.. |
|||
Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
ExxonMobil Santoprene® 271-80 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
ExxonMobil Santoprene® 273-40 Thermoplastic Elastomer A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Clamp Pressure | 41.0 - 69.0 MPa | 5950 - 10000 psi | |
ExxonMobil Santoprene® 8281-65MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
ExxonMobil Santoprene® 271-73 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
ExxonMobil Santoprene® 211-80 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
ExxonMobil Vyram™ 9201-65 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
ExxonMobil Santoprene® 221-87 Thermoplastic Elastomer
(discontinued **) A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
ExxonMobil Santoprene® 101-80 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Clamp Pressure | 41.4 - 68.9 MPa | 6000 - 10000 psi | |
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |