Processing Properties Metric English Comments
Clamp Pressure <= 6.89 MPa
<= 1000 psi
Molding Pressure
Premix Premi-Glas® 1261-28 VE Glass Reinforced Vinyl Ester TMC
Description: Premi-Glas® 1261-28 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Excellent thermal stability an..
Clamp Pressure <= 6.89 MPa
<= 1000 psi
Molding Pressure
Premix Premi-Glas® 1266 (Injection Compression Molded) Glass Reinforced TMC
Description: Premi-Glas® 1266 is a glass reinforced thermoset molding compound designed for automotive under the hood applications. Key features and benefits: Designed for Injection or Injection/Co..
Clamp Pressure <= 6.89 MPa
<= 1000 psi
Molding Pressure
Premix Premi-Glas® 1268 Fiberglass Reinforced Thermoset Thick Molding Compound
Premi-Glas® 1268 is a fiberglass reinforced thermoset thick molding compound for composite power train applications such as valve covers and timing gear covers.Key features and benefits are:Ideal f..
Clamp Pressure <= 6.89 MPa
<= 1000 psi
Molding Pressure
Premix Premi-Glas® 8101 Glass Reinforced Polyester BMC
Description: Premi-Glas® 8101 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits: Ex..