Processing Properties | Metric | English | Comments |
---|---|---|---|
Annealing Temperature | 950 - 1050 °C | 1740 - 1920 °F | Stress Relief Annealing |
Outokumpu SAF 2304® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Annealing Temperature | 950 - 1050 °C | 1740 - 1920 °F | Quench Annealing |
Outokumpu SAF 2304® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |