Processing Properties | Metric | English | Comments |
---|---|---|---|
Annealing Temperature | 649 - 760 °C | 1200 - 1400 °F | Sub-critical anneal |
Schmolz + Bickenbach 416 Stainless Steel Bar Description: Ugitech’s 416 is free machining martensitic grade. The unique production process—developed exclusively by Ugitech—results in a product that delivers superior productivity.. |
|||
Annealing Temperature | 649 - 760 °C | 1200 - 1400 °F | Sub-critical anneal |
Schmolz + Bickenbach 416RS Stainless Steel Bar Description: Ugitech’s 416RS is a low sulfur pre-hardened chrome bearing martensitic stainless steel specifically designed for the precision rifle barrel industry. The 416RS chemistry is balanc.. |
|||
Annealing Temperature | 650 - 825 °C | 1200 - 1520 °F | |
California Fine Wire Copper, 27% Nickel Clad All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |