Polymer Property : Annealing Temperature = 1130 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Annealing Temperature 610 - 649 °C
1130 - 1200 °F
Soft; Cooling: Furnace 20°F/hour to 930°F then air cool; < 220 HB
Schmolz + Bickenbach Cryodur® 2357(S-7) Cold Work Die Steel
Description: Cryodur 2357 is a shock resistant tool steel with excellent toughness and high strength; Suitable for cold and hot work applications up to 1000 °F; and Supplied in the annealed conditi..
Annealing Temperature 610 - 650.0 °C
1130 - 1202 °F
Soft; Cooling: Furnace; <260 HB
Schmolz + Bickenbach Cryodur® 2767 Cold Work Die Steel
Description: High hardenability and toughness, highly suitable for polishing, texturing and EDM machining. We recommend the use of Cryodur® 2767 (ERS) for extreme demandsApplications: Cutlery dies,..