Polymer Property : Annealing Temperature = 760 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Annealing Temperature 649 - 760 °C
1200 - 1400 °F
Sub-critical anneal
Schmolz + Bickenbach 416 Stainless Steel Bar
Description: Ugitech’s 416 is free machining martensitic grade. The unique production process—developed exclusively by Ugitech—results in a product that delivers superior productivity..
Annealing Temperature 649 - 760 °C
1200 - 1400 °F
Sub-critical anneal
Schmolz + Bickenbach 416RS Stainless Steel Bar
Description: Ugitech’s 416RS is a low sulfur pre-hardened chrome bearing martensitic stainless steel specifically designed for the precision rifle barrel industry. The 416RS chemistry is balanc..