Processing Properties | Metric | English | Comments |
---|---|---|---|
Annealing Temperature | 830.0 - 860 °C | 1526 - 1580 °F | Soft; Cooling: Furnace; < 250HB |
Schmolz + Bickenbach Cryodur® 2990 Cold Work Die Steel Description: Newly developed ledeburitic cold-work steel with high hardness, good toughness and high tempering resistance combined with high wear resistance.Applications: Cutting and punching tools .. |