Processing Properties | Metric | English | Comments |
---|---|---|---|
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning A Compound Antifoam 100% active silicone fluid containing a suspension of finely powdered silica to enhance its defoaming efficiency.Information provided by Dow Corning |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning H-10 ANTIFOAM EMULSION 10 percent active, water dilutable silicone emulsion designed to control foam in water based industrial processes.Information provided by Dow Corning |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning MOLYKOTE® G-0103 GREASE Mineral base multi-service grease designed for extended lubrication of bearingsInformation provided by Dow Corning |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning OS-120 Information provided by Dow Corning |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning SILASTIC® LS 5-2040 FLUOROSILICONE RUBBER 40 Durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning SILASTIC® LS-2380 FLUOROSILICONE RUBBER 70 Durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning SILASTIC® LT-40 SILICONE RUBBER 40 Durometer, translucent, Aviation Component grade, Uncatalysed Silicone Rubber BaseInformation provided by Dow Corning |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning SYL-OFF® 297 ANCHORAGE ADDITIVE Syl-Off® 297 Anchorage Additive is a mixture of reactive silanes that is used to improve abrasion resistance and adhesion of the cured coating to the substrate.Information provided by Dow Corning |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning XIAMETER® PMCPPMX-200 100,000CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 100,000CS. 100% active, 100,000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning Z-6026 SILANE Dow Corning® Z-6026 Silane is a chemically reactive material composed of an amino-alkyltrimethoxysilane and a polyol diluted to 40% by weight in methanol. Chemically, it is similar to Dow Corning®.. |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning Z-6070 SILANE Dow Corning Z-6070 Silane is a chemical monomer that reacts with water to form a silanetriol and methanol. The silanol that is formed is able to condense with available hydroxyl groups on the surfac.. |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning Z-6079 SILANE DOW CORNING Z6079 Silane is useful in protecting OH and SH functionality of complex molecules, permitting other sites to be selectively reacted.Information provided by Dow Corning |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning Z-6121 SILANE Dow Corning® Z-6121 Silane is a multi-purpose silane adhesion promoter recommended for use with epoxy coatings, silicone resin-based coatings and alkyd finishes.Information provided by Dow Corning |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning Z-6518 SILANE Dow Corning® Z-6518 Silane is an organofunctional reactive silane. The product have a vinyl reactive organic group and a trimethoxysilyl or triethoxysilyl reactive inorganic group. Dow Corning® Z-.. |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning 1400 Antifoam 100% active silicone fluid containing a suspension of finely powdered silica to enhance its defoaming efficiency.Information provided by Dow Corning |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning 1500 Antifoam 100% active silicone fluid containing a suspension of finely powdered silica to enhance its defoaming efficiency. Food grade antifoam.Information provided by Dow Corning |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning 203 Fluid 100% active alkylaryl polysiloxane fluid.Information provided by Dow Corning |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning 204 Fluid 100% active alkylaryl polysiloxane fluid.Information provided by Dow Corning |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning 230 Fluid 100% active alkylaryl polysiloxane fluid.Information provided by Dow Corning |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning SILASTIC® LS 5-8760 FLUOROSILICONE RUBBER 60 Durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning SILASTIC® LS-2860 FLUOROSILICONE RUBBER 60 Durometer, off-white, uncatalysed, moulding grade fluorosilicone baseInformation provided by Dow Corning |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning XIAMETER® PMCPPMX-200 60,000CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 60,000CS. 100% active, 60,000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning Z-6020 SILANE Aminoethylaminopropyltrimethoxysilane - H2NC2H4NHC3H6-Si(OCH3)3 Coupling agent for many thermoset and thermoplastic resins with glass or mineral fillers.Information provided by Dow Corning |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning Z-6042 SILANE ?-Glycidoxypropyl(methyl) diethoxysilaneInformation provided by Dow Corning |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning Z-6106 SILANE Dow Corning® Z-6106 Silane acts as a coupling agent designed to promote adhesion of two dissimilar materials. It can be used to bond a polymeric coating or adhesive to an inorganic substrate or to .. |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning 2-5088 Wax Silicone wax (siloxane backbone with pendant C30 alkyl groups attached). In home and auto care applications, it combines the shine and durability associated with hard waxes, with features closer to .. |
|||
Shelf Life | 36.0 Month @Temperature 7.22 °C |
36.0 Month @Temperature 45.0 °F |
From date of manufacture |
Arlon 99790N010 0.010" (0.254 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Side 1: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassThis data represents typical values for the production material. The data should not be used to write,.. |
|||
Shelf Life | 36.0 Month @Temperature 15.0 - 27.0 °C |
36.0 Month @Temperature 59.0 - 80.6 °F |
|
3M PN8017 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |
|||
Shelf Life | 36.0 Month @Temperature 15.0 - 27.0 °C |
36.0 Month @Temperature 59.0 - 80.6 °F |
|
3M PN8019 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |
|||
Shelf Life | 36.0 Month | 36.0 Month | |
Dow Corning 3074 INTERMEDIATE Reactive silicone intermediate for coil coatings, appliance finishes and other finishes where improved heat or weathering resistance is needed. Typically reacted with saturated polyesters to form si.. |