Processing Properties | Metric | English | Comments |
---|---|---|---|
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning 700 INDUSTRIAL GRADE SILICONE SEALANT General industrial sealing and adhesive applicationsInformation provided by Dow Corning |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning 733 GLASS & METAL SEALANT Conventional acetoxy RTV sealant with adhesion promoterInformation provided by Dow Corning |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning 736 HEAT RESISTANT/SEALANT Red RTV adhesive/sealant for temperatures up to 600F/315CInformation provided by Dow Corning |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning 786 SILICONE MILDEW RESISTANT SEALANT Dow Corning® 786 Silicone Sealant is designed to seal nonporous surfaces around showers, tubs, sinks and plumbing fixtures where conditions of high humidity and temperature extremes exist.Informati.. |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning Q4-3667 Fluid Silicone polyether (glycol) copolymer.Information provided by Dow Corning |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning XIAMETER® PMCPPMX-0244 Cyclotetrasiloxane Is chemically equivalent to DOW CORNING® 244 FLUID. This product is a volatile methylsiloxane fluid, clear, odorless, VOC-exempt, low toxicity, low surface tension and evaporates completely at room.. |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning XIAMETER® PMCPPMX-0245 Cyclopentasiloxane Is chemically equivalent to DOW CORNING® 245 FLUID. This product a volatile, low viscosity cyclopentasiloxane fluid for use in skincare, suncare, color cosmetics, hair care, and antiperspirant / de.. |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning XIAMETER® PMCPPMX-0246 Cyclohexasiloxane Is chemically equivalent to DOW CORNING® 246 FLUID. This product is a volatile, low viscosity cyclohexasiloxane fluid for use in skincare, suncare, color cosmetics, hair care, and antiperspirant / .. |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning XIAMETER® PMCPPMX-0344 Cyclosiloxane Blend Is chemically equivalent to DOW CORNING® 344 FLUID. A volatile methylsiloxane fluid, clear, odorless, VOC-exempt, low toxicity, low surface tension, evaporates completely at room temperatureInforma.. |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning XIAMETER® PMCPPMX-0345 Cyclosiloxane Blend Is chemically equivalent to DOW CORNING® 345 FLUID. A blend of polydimethylcyclosiloxanes composed mainly of cyclopentasiloxane and cyclohexasiloxane for use in skincare, suncare, color cosmetics, .. |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning 1248 Fluid Silicone glycol graft copolymer with secondary hydroxyl functionality. The polymer has a combination of organoreactivity from the glycol group as well as properties typical of a polydimethylsiloxane.. |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning 1503 Fluid A blend of an ultra high viscosity dimethiconol in a low viscosity dimethicone fluid for use in skincare, woundcare, scar therapy, suncare, and color cosmetic applications.Information provided by Do.. |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning 193C Fluid Dow Corning ® 193C Fluid is a silicone glycol copolymer.Information provided by Dow Corning |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning 2-1912 FLUID Blend of polydimethylsiloxane and high molecular weight silicone resin. Reactive silicone fluids used for silica treatment.Information provided by Dow Corning |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning 2-2617 Diesel Antifoam 100% active polysilicone polyether copolymer, used to control foam in diesel fuel.Information provided by Dow Corning |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning 2-2647 Performance Modifier Surface active silicone designed for reducing surface tension in silicone emulsions and improving drainage in pulp brownstock washing.Information provided by Dow Corning |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning 593 FLUID Blend of polydimethylsiloxane and high molecular weight silicone resin.Information provided by Dow Corning |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning DM2 Demulsifier Silicone polyether, acts as a performance booster for crude oil emulsion breakers.Information provided by Dow Corning |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning DM3 Demulsifier Silicone polyether, acts as a performance booster for crude oil emulsion breakers.Information provided by Dow Corning |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning DM6 Demulsifier Silicone polyether, acts as a performance booster for crude oil emulsion breakers.Information provided by Dow Corning |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning 3527 RELEASE AGENT Blend of polydimethylsiloxane and high molecular weight silicone resin.Information provided by Dow Corning |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning 43 Paperaid Dow Corning® Paperaid 43 is 100% solids silicone polyether. Suitable as antifoam in the production of rosin size.Information provided by Dow Corning |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning 5200 Formulation Aid An alkylmethyl siloxane copolyol designed to prepare stable water-in-oil emulsions.Information provided by Dow Corning |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning 5329 Modifier A polyether functional siloxaneInformation provided by Dow Corning |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning 54 Additive Provides mar resistance, slip, leveling and gloss. Also aids in pigment dispersion.Information provided by Dow Corning |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning 5604 Performance Modifier Surface active silicone designed for reducing surface tension in silicone emulsions and improving drainage in pulp brownstock washing.Information provided by Dow Corning |
|||
Shelf Life | 30.0 Month | 30.0 Month | |
Dow Corning 29 Additive Enhances flow, leveling and gloss; also imparts mar resistance and anti-blocking.Information provided by Dow Corning |