Processing Properties | Metric | English | Comments |
---|---|---|---|
Shelf Life | 3.00 Month | 3.00 Month | |
Gwent Electronic Materials C2021031D3 Electrode Ink Electrode Ink C2021031D3 is a Silver Palladium (90/10) electrode ink, designed for use with PVB Tape. It has been specifically formulated for use with PZT ceramics.The ink is in a ready to use form.. |
|||
Shelf Life | 3.00 Month | 3.00 Month | at 20°C maximum |
Gwent Electronic Materials C2050712D58 Silver Ink for ITO Substrates This product is based on a unique curing process that results in the low temperature formation of a thermosetting polymer. Inks containing these polymers combine excellent chemical, environmental a.. |
|||
Shelf Life | 3.00 Month | 3.00 Month | |
Gwent Electronic Materials C60531D1 Silver / Silver Chloride Paste C60531D1 has a ratio of Silver to Silver Chloride of 90/10. This is used for reference electrodes in Medical Diagnostics, Environmental Sensor and the "Agri-Food" Industries. It forms part of a fa.. |
|||
Shelf Life | 3.00 Month | 3.00 Month | |
Gwent Electronic Materials D2020823D2 Polymer Dielectric This material is a blue colored screen printable polymer Dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode... |
|||
Shelf Life | 3.00 Month | 3.00 Month | |
Gwent Electronic Materials D2030210D1 Polymer Dielectric This material is a black colored screen printable polymer Dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode.. |
|||
Shelf Life | 3.00 Month | 3.00 Month | |
Lucite International Colacryl ® TS1778 Acrylic Solution Resin Colacryl TS 1778 is a self cross-linking acrylic copolymer designed for adhesive applications. Once dried, a film cast from this product remains permanently tacky.Suggested Uses: Pressure-sensitiv.. |
|||
Shelf Life | 3.00 Month | 3.00 Month | at 25°C |
Tipco Tipwood® 50 EX 50EX Description: Tipwood® is a Wood-Fiber Reinforced, Heat Stabilized Polypropylene Compound specially developed by Tipco for Automobile Interiors and Appliance Fascia Applications.Features: Environmen.. |
|||
Shelf Life | 3.00 Month @Temperature -40.0 °C |
3.00 Month @Temperature -40.0 °F |
|
Loctite® 3564 Fast flow epoxy, moderate CTE and Tg Fast Flow Underfill COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.Loctite® Underfills and Encapsulants imp.. |
|||
Shelf Life | 3.00 Month @Temperature -40.0 °C |
3.00 Month @Temperature -40.0 °F |
|
Loctite® 3534 Glob Top Encapsulant COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.Loctite® Underfills and Encapsulants imp.. |
|||
Shelf Life | 3.00 Month | 3.00 Month | |
Dow Corning HV 1760/80 SILICONE RUBBER NATURAL 80 Shore hardness high consistency silicone rubber with fast cure system and excellent tracking and erosion resistanceInformation provided by Dow Corning |
|||
Shelf Life | 3.00 Month | 3.00 Month | Moisture absorption after extended storage |
Fainplast Compounds EVAtech 805S Ethylene Vinyl Acetate Foam EVA (ethylene-vinyl acetate) designed for the production of crosslinked expanded products using injection technology.Information provided by Fainplast Compounds |
|||
Shelf Life | 3.00 Month @Temperature 30.0 °C |
3.00 Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
Fainplast Compounds Hax™ HFC 087/2 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Bedding for tandem extrusion onlyInformation provided by Fainplast Compounds |
|||
Shelf Life | 3.00 Month @Temperature 30.0 °C |
3.00 Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
Fainplast Compounds Hax™ HFX 507 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing; Insulation; easy processingInformation provided.. |
|||
Shelf Life | 3.00 Month @Temperature 30.0 °C |
3.00 Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
Fainplast Compounds Hax™ HFX 515 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing, InsulationInformation provided by Fainplast Com.. |
|||
Shelf Life | 3.00 Month @Temperature 30.0 °C |
3.00 Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
Fainplast Compounds Hax™ HF 225F Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Sheathing, high flexibilityInformation provided by Fainplast Compounds |
|||
Shelf Life | 3.00 Month @Temperature 30.0 °C |
3.00 Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
Fainplast Compounds Hax™ HFC 0108 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Bedding, designed to meet BS 6724Information provided by Fainplast Compounds |
|||
Shelf Life | 3.00 Month @Temperature 30.0 °C |
3.00 Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
Fainplast Compounds Hax™ HFX 521 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Oil resistant sheathingInformation provided by Fainplast C.. |
|||
Shelf Life | 3.00 Month @Temperature 4.44 °C |
3.00 Month @Temperature 40.0 °F |
From date of manufacture |
Arlon 15880T025 0.025" (0.635 mm) Uncured, Unsupported Silicone Rubber on a Mylar Carrier Design/Construction:Side 1: Uncatalyzed, Unsupported Silicone Rubber on a Mylar CarrierAppearance: Clear silicone gum on polymer filmThis data represents typical values for the production material. .. |
|||
Shelf Life | 3.00 Month @Temperature 4.44 °C |
3.00 Month @Temperature 40.0 °F |
From date of manufacture |
Arlon 30400N060 0.060" (1.52 mm) Uncured Silicone Rubber Design/Construction: Interleave 1: KodacelProduct: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Translucent silicone rubber on polymer linerThis data represents typical values for .. |
|||
Shelf Life | 3.00 Month @Temperature 4.44 °C |
3.00 Month @Temperature 40.0 °F |
|
Arlon 30400R040 0.04" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should.. |
|||
Shelf Life | 3.00 Month @Temperature 21.1 °C |
3.00 Month @Temperature 70.0 °F |
From date of manufacture |
Arlon 32400R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier Design/Construction:Side 1: Uncured Silicone RubberCarrier: PETInterleave: PolyethyleneAppearance: Red silicone rubber on polymer linerThis data represents typical values for the production material.. |
|||
Shelf Life | 3.00 Month @Temperature 4.44 °C |
3.00 Month @Temperature 40.0 °F |
From date of manufacture |
Arlon 75400R045 0.045" (1.14 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info.. |
|||
Shelf Life | 3.00 Month @Temperature 23.9 °C |
3.00 Month @Temperature 75.0 °F |
From date of manufacture |
Arlon P29514R020 0.0205" (0.521 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassAppearance: Red silicone rubber on fiberglass fabric.This data represents typical values for the product.. |
|||
Shelf Life | 3.00 Month @Temperature 7.22 °C |
3.00 Month @Temperature 45.0 °F |
From date of manufacture |
Arlon P30670R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Uncured Silicone Rubber Substrate: Style 1165 FiberglassAppearance: Red silicone gum on fiberglass with polymer release linersThis data represents typical values for the.. |
|||
Shelf Life | 3.00 Month @Temperature 4.44 °C |
3.00 Month @Temperature 40.0 °F |
From date of manufacture |
Arlon R35640T003 0.003" (0.0762 mm) Uncured Silicone Rubber with Polyethylene Naphthalate Substrate Design/Construction:Liner: Polyester Side 1: Uncured Silicone RubberSubstrate: Polyethylene NaphthalateAppearance: Gray gum on glass fiber fabricThis data represents typical values for the productio.. |
|||
Shelf Life | 3.00 Month @Temperature 4.44 - 10.0 °C |
3.00 Month @Temperature 40.0 - 50.0 °F |
From date of manufacture |
Arlon Thermabond® R36200A008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated Fiberglass Appearance: Blue silicone gumThis data represents typical values for the production material. The d.. |
|||
Shelf Life | 3.00 Month | 3.00 Month | |
Gwent Electronic Materials C2030519P5 Carbon Graphite Ink This Carbon Graphite Ink is designed to be used for screen printing working electrodes. These electrodes when used in conjunction with NAD+/NADH dependent dehydrogenase enzymes, enable the detection.. |
|||
Shelf Life | 3.00 Month @Temperature 7.22 °C |
3.00 Month @Temperature 45.0 °F |
From date of manufacture |
Arlon 32400N030 0.030" (0.762 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PET Appearance: Translucent silicone rubber on polymer linerThis data represents typical values for the productio.. |
|||
Shelf Life | 3.00 Month @Temperature 4.44 °C |
3.00 Month @Temperature 40.0 °F |
From date of manufacture |
Arlon 32400N060 0.060" (1.52 mm) Uncured Silicone Rubber Design/Construction: Interleave 1: PET carrierSide 1: Uncured Silicone RubberInterleave 2 : PE carrierAppearance: Translucent silicone rubber on polymer linerThis data represents typical values for .. |
|||
Shelf Life | 3.00 Month | 3.00 Month | |
Gwent Electronic Materials C2010809D3 Silver Ink Silver Ink C2010809D3 is designed for printing via, when screen printed onto LTCC tape. It is compatible with other members of the GEM range of Silver LTCC Inks and most LTCC tape systems on the ma.. |