Processing Properties | Metric | English | Comments |
---|---|---|---|
Shelf Life | 3.00 Month | 3.00 Month | at room temperature |
Permabond TA4592 Toughened Acrylic Adhesive PERMABOND® TA4592 is a two component structural acrylic adhesive ideal for bonding magnets and ferrites for electric motors on fast-moving production lines. Permabond® TA4592 provides high strengt.. |
|||
Shelf Life | 3.00 Month | 3.00 Month | |
Gwent Electronic Materials C2010829D2 Silver Ink Silver Ink C2010829D2 is a high definition silver ink for LTCC tape. It is compatible with other members of the GEM range of Silver LTCC Inks and most LTCC tape systems on the market.The ink has be.. |
|||
Shelf Life | 3.00 Month | 3.00 Month | |
Gwent Electronic Materials D50706D2 Polymer Dielectric This material is a cream colored screen printable polymer Dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode.. |
|||
Shelf Life | 3.00 Month | 3.00 Month | with proper storage |
Stanelco Bioplast® Wrap 100 Biodegradable Plastic Bioplast Wrap 100 is a plasticiser-free thermoplastic material which allows the production of films with coated paper-like properties. Wrap 100 is an excellent, eco-friendly alternative to laminated.. |
|||
Shelf Life | 3.00 - 6.00 Month @Temperature 23.9 °C |
3.00 - 6.00 Month @Temperature 75.0 °F |
in unopened containers |
Master Bond EP21TDCNFL Two Component Nickel Conductive Epoxy Adhesive Master Bond Polymer System EP21TDCNFL is a two component, nickel filled, electrically conductive system for high performance bonding and sealing formulated to cure at room temperature or more rapidl.. |
|||
Shelf Life | 3.00 Month @Temperature 23.9 °C |
3.00 Month @Temperature 75.0 °F |
in syringe |
Master Bond EP21TDCS Two Component Silver Conductive Epoxy Adhesive Master Bond Polymer System EP21TDCS is a two component, silver filled, electrically conductive adhesive for high performance bonding and sealing formulated to cure at room temperature or more rapidl.. |
|||
Shelf Life | 3.00 - 6.00 Month @Temperature 23.9 °C |
3.00 - 6.00 Month @Temperature 75.0 °F |
in original unopened containers |
Master Bond Supreme 10HTCL Epoxy for Cryogenic Applications Description: Master Bond Supreme 10HTCL features a blend of performance properties including both high shear and peel strengths along with convenient handling. This one component system is formulate.. |
|||
Shelf Life | 3.00 Month | 3.00 Month | at 25°C |
Tipco Tipwood® 50 EX 50EX Description: Tipwood® is a Wood-Fiber Reinforced, Heat Stabilized Polypropylene Compound specially developed by Tipco for Automobile Interiors and Appliance Fascia Applications.Features: Environmen.. |
|||
Shelf Life | 3.00 Month | 3.00 Month | |
Tra-Con Tra-Bond 724-17GR Polyurethane Adhesive TRA-BOND 724-17GR premixed and frozen, polyurethane adhesive is designed for good adhesion, providing strong resilient bonds to a wide variety of substrates, including aluminum, solder, nylon, mylar.. |
|||
Shelf Life | 3.00 Month @Temperature -40.0 °C |
3.00 Month @Temperature -40.0 °F |
|
Loctite® 3533 Low viscosity fill encapsulant Fill Encapsulant COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.Loctite® Underfills and Encapsulants imp.. |
|||
Shelf Life | 3.00 Month @Temperature -40.0 °C |
3.00 Month @Temperature -40.0 °F |
|
Loctite® 3564 Fast flow epoxy, moderate CTE and Tg Fast Flow Underfill COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.Loctite® Underfills and Encapsulants imp.. |
|||
Shelf Life | 3.00 - 6.00 Month | 3.00 - 6.00 Month | |
Master Bond EP21TDCSLO Two Component Silver Conductive Epoxy Adhesive Master Bond Polymer System EP21TDCS-LO is a two component, silver filled, electrically conductive adhesive for high performance bonding and sealing formulated to cure at room temperature or more rap.. |
|||
Shelf Life | 3.00 Month @Temperature 30.0 °C |
3.00 Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
Fainplast Compounds Hax™ HF 411 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:SheathingInformation provided by Fainplast Compounds |
|||
Shelf Life | 3.00 Month @Temperature 30.0 °C |
3.00 Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
Fainplast Compounds Hax™ HFC 0115/1 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Bedding for tandem extrusion onlyInformation provided by Fainplast Compounds |
|||
Shelf Life | 3.00 Month @Temperature 30.0 °C |
3.00 Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
Fainplast Compounds Hax™ HFX 505 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing; InsulationInformation provided by Fainplast Com.. |
|||
Shelf Life | 3.00 Month @Temperature 30.0 °C |
3.00 Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
Fainplast Compounds Hax™ HFX 509 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Insulation for solar cablesInformation provided by Fainpla.. |
|||
Shelf Life | 3.00 Month @Temperature 30.0 °C |
3.00 Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
Fainplast Compounds Hax™ HF 045/16M Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Sheathing, insulation, low shrinkageInformation provided by Fainplast Compounds |
|||
Shelf Life | 3.00 Month @Temperature 30.0 °C |
3.00 Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
Fainplast Compounds Hax™ HF 215 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:High flame retardancy, improved processabilityInformation provided by Fainplast Compound.. |
|||
Shelf Life | 3.00 Month @Temperature 30.0 °C |
3.00 Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
Fainplast Compounds Hax™ HF 225F Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Sheathing, high flexibilityInformation provided by Fainplast Compounds |
|||
Shelf Life | 3.00 Month @Temperature 30.0 °C |
3.00 Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
Fainplast Compounds Hax™ HF 4024 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Insulation and sheathing, improved processabilityInformation provided by Fainplast Compo.. |
|||
Shelf Life | 3.00 Month @Temperature 30.0 °C |
3.00 Month @Temperature 86.0 °F |
Moisture absorption after extended storage |
Fainplast Compounds Hax™ HFC 0108 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Bedding, designed to meet BS 6724Information provided by Fainplast Compounds |
|||
Shelf Life | 3.00 Month @Temperature 21.1 °C |
3.00 Month @Temperature 70.0 °F |
From date of manufacture |
Arlon 32400R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier Design/Construction:Side 1: Uncured Silicone RubberCarrier: PETInterleave: PolyethyleneAppearance: Red silicone rubber on polymer linerThis data represents typical values for the production material.. |
|||
Shelf Life | 3.00 Month @Temperature 21.1 °C |
3.00 Month @Temperature 70.0 °F |
|
Arlon 51044R020 0.020" Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Semi-cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material and should no.. |
|||
Shelf Life | 3.00 Month @Temperature 23.9 °C |
3.00 Month @Temperature 75.0 °F |
From date of manufacture |
Arlon R35948R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberThis data re.. |
|||
Shelf Life | 3.00 Month @Temperature 4.44 - 10.0 °C |
3.00 Month @Temperature 40.0 - 50.0 °F |
From date of manufacture |
Arlon Thermabond® R36200A008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated Fiberglass Appearance: Blue silicone gumThis data represents typical values for the production material. The d.. |
|||
Shelf Life | 3.00 Month @Temperature 23.9 °C |
3.00 Month @Temperature 75.0 °F |
From date of manufacture |
Arlon R33889R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Layer-on-Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information .. |
|||
Shelf Life | 3.00 Month | 3.00 Month | |
Gwent Electronic Materials C2030519P5 Carbon Graphite Ink This Carbon Graphite Ink is designed to be used for screen printing working electrodes. These electrodes when used in conjunction with NAD+/NADH dependent dehydrogenase enzymes, enable the detection.. |
|||
Shelf Life | 3.00 Month @Temperature 7.22 °C |
3.00 Month @Temperature 45.0 °F |
From date of manufacture |
Arlon 32400N030 0.030" (0.762 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PET Appearance: Translucent silicone rubber on polymer linerThis data represents typical values for the productio.. |
|||
Shelf Life | 3.00 - 6.00 Month @Temperature 23.9 °C |
3.00 - 6.00 Month @Temperature 75.0 °F |
in original unopened containers |
Master Bond Supreme 10HTFL One Part Epoxy Cures at 250°F Description: Master Bond Polymer System Supreme 10HTFL features a blend of physical properties including outstanding peel strength, very high shear strength and a wide service temperature range of 4.. |