Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Air Flow Rate | 22.7 - 28.3 l/min | 0.800 - 1.00 ft³/min (CFM) | per lb/hour resin processed |
MRC Polymers MAXNITE™ 500 GF15 PET, 15% Glass Fiber Filled
(discontinued **) Information provided by MRC Polymers Inc. |
|||
Drying Air Flow Rate | 22.7 - 28.3 l/min | 0.800 - 1.00 ft³/min (CFM) | per lb/hour resin processed |
MRC Polymers EMAREXâ„¢ 300 GF33 Nylon 6, 33% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Drying Air Flow Rate | 22.7 - 28.3 l/min | 0.800 - 1.00 ft³/min (CFM) | per lb/hour resin processed |
MRC Polymers EMAREXâ„¢ 300 GF43 Nylon 6, 43% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Drying Air Flow Rate | 22.7 - 28.3 l/min | 0.800 - 1.00 ft³/min (CFM) | per lb/hour resin processed |
MRC Polymers EMAREXâ„¢ 400 GF13 Nylon 6/6, 13% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Drying Air Flow Rate | 22.7 - 28.3 l/min | 0.800 - 1.00 ft³/min (CFM) | per lb/hour resin processed |
MRC Polymers MAXTELâ„¢ 600 GF20 TPO, 20% Glass Fiber Filled For automotive exterior applications. Excellent process ability and dimensional stability.Internal and external lubricants can be addedCan be UV StabilizedInformation provided by MRC Polymers Inc. |
|||
Drying Air Flow Rate | 22.7 - 28.3 l/min | 0.800 - 1.00 ft³/min (CFM) | per lb/hour resin processed |
MRC Polymers MAXTELâ„¢ 600 GF30 TPO, 30% Glass Fiber Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Drying Air Flow Rate | 22.7 - 28.3 l/min | 0.800 - 1.00 ft³/min (CFM) | per lb/hour resin processed |
MRC Polymers NAXALOYâ„¢ 770 ABS + PC Alloy Impact modifiedAvailable in Natural, Black, and GrayCan be Colored (Masterbatch)Low temperature ductility and impact modifiedCan be UV StabilizedInternal and external lubricant can be addedInformati.. |
|||
Drying Air Flow Rate | 22.7 - 28.3 l/min | 0.800 - 1.00 ft³/min (CFM) | per lb/hour resin processed |
MRC Polymers NAXALOYâ„¢ 770 GF10 ABS+PC Alloy, 10% Glass Fiber Filled Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Drying Air Flow Rate | 22.7 - 28.3 l/min | 0.800 - 1.00 ft³/min (CFM) | per lb/hour resin processed |
MRC Polymers NAXALOYâ„¢ 770 GF16 ABS+PC Alloy, 16% Glass Fiber Filled Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Drying Air Flow Rate | 22.7 - 28.3 l/min | 0.800 - 1.00 ft³/min (CFM) | per lb/hour resin processed |
MRC Polymers NAXALOYâ„¢ 780 GF11 PC+PBT Polyester Blend, 11% Glass Fiber Filled Good chemical resistance, impact and heat resistanceAvailable in Black OnlyCan be UV StabilizedInternal and external lubricant can be added.Information provided by MRC Polymers Inc. |
|||
Drying Air Flow Rate | 22.7 - 28.3 l/min | 0.800 - 1.00 ft³/min (CFM) | per lb/hour resin processed |
MRC Polymers NAXALOYâ„¢ 780 PC+PBT Polyester Blend Good chemical resistance, impact and heat resistance.Information provided by MRC Polymers Inc. |
|||
Drying Air Flow Rate | 22.7 - 28.3 l/min | 0.800 - 1.00 ft³/min (CFM) | per lb/hour resin processed |
MRC Polymers NAXALOYâ„¢ 793A3 GF10 PC and Polyester Blend, 10% Glass Fiber Filled 793 GF10 is available in natural and custom colors, internal and external lubricants, UV stabilizer and other modifications.Information provided by MRC Polymers Inc. |
|||
Drying Air Flow Rate | 22.7 - 28.3 l/min | 0.800 - 1.00 ft³/min (CFM) | per lb/hour resin processed |
MRC Polymers EMAREXâ„¢ 400 GF33 Nylon 6/6, 33% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Drying Air Flow Rate | 22.7 - 28.3 l/min | 0.800 - 1.00 ft³/min (CFM) | per lb/hour resin processed |
MRC Polymers NAXELLâ„¢ PC110-919 General Purpose Polycarbonate, Medium High MFR Polycarbonate for colorable productsMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedCan be clear to color matchedNot for products that req.. |
|||
Drying Air Flow Rate | 22.7 - 28.3 l/min | 0.800 - 1.00 ft³/min (CFM) | per lb/hour resin processed |
MRC Polymers NAXELLâ„¢ PC210MR General Purpose Polycarbonate, Medium MFR, with Release Medium melt without impact modificationMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedGenerally for black and gray colors onlyFR package .. |
|||
Drying Air Flow Rate | 22.7 - 28.3 l/min | 0.800 - 1.00 ft³/min (CFM) | per lb/hour resin processed |
MRC Polymers NAXELLâ„¢ PC23M-10G General Purpose Polycarbonate, 10% Glass Fiber Filled, Low Viscosity Can be impact modifiedInternal and external lubricant can be addedBlack onlyInformation provided by MRC Polymers Inc. |
|||
Drying Air Flow Rate | 22.7 - 28.3 l/min | 0.800 - 1.00 ft³/min (CFM) | per lb/hour resin processed |
MRC Polymers NAXELLâ„¢ PC23MS Polycarbonate, Impact Modified, High MFR, EZ Flow Economy GradeImpact modifiedCan be UV stabilizedGenerally for black onlyInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Drying Air Flow Rate | 22.7 - 28.3 l/min | 0.800 - 1.00 ft³/min (CFM) | per lb/hour resin processed |
MRC Polymers NAXELLâ„¢ PC429HHI Polycarbonate, Impact Modified, High MFR, EZ Flow Good Property RetentionHeat and Dimensional StabilityHigh Melt Impact ModifiedMFR can be modified between 10 to 26 g/10minsCan be UV stabilizedGenerally for natural, colorable and can go blackIntern.. |