Processing Properties | Metric | English | Comments |
---|---|---|---|
Dew Point | -33.9 °C | -29.0 °F | Average value: -33.9 °C Grade Count:4 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |