Processing Properties | Metric | English | Comments |
---|---|---|---|
Roll Temperature | 140 - 160 °C | 284 - 320 °F | Hotmelt Coating Multi Roller |
EMS-Griltech Griltex® D 1500A Copolyamide Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Roll Temperature | 140 - 160 °C | 284 - 320 °F | Hotmelt Coating Multi Roller |
EMS-Griltech Griltex® D 1516A Heat Stabilized Copolyamide Hotmelt Adhesive (Technical Applications) GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides for excellent r.. |
|||
Roll Temperature | 140 - 180 °C | 284 - 356 °F | Hotmelt Coating Multi Roller |
EMS-Griltech Griltex® D 1531E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Roll Temperature | 140 - 160 °C | 284 - 320 °F | Hotmelt Coating Multi Roller |
EMS-Griltech Griltex® D 1539E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |