Polymer Property : Roll Temperature = 21.1 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 3160 Thermoplastic Elastomer
A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3160 can be processed by injection molding or extrusion for ap..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 3439D Thermoplastic Elastomer
A NSF certified, high hardness, multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by injectio..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 3440 Thermoplastic Elastomer
A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 3445D Thermoplastic Elastomer
A NSF certified, high hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inje..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 3445DN Thermoplastic Elastomer
A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 3450 Thermoplastic Elastomer
A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 3460 Thermoplastic Elastomer
A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 3470 Thermoplastic Elastomer
A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 3470N Thermoplastic Elastomer
A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 4145 Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4145 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 4155 Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4155 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 4165 Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4165 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 4175 Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4175 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 4180 Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4180 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 4190 Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4190 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 4370 Thermoplastic Elastomer
A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4370 is a flame retardant, soft hardness grade exhibiting exceptional chemical resistance, compression set..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 4380 Thermoplastic Elastomer
A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4380 is a flame retardant, medium hardness grade processing exceptional chemical resistance, compression s..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 4390 Thermoplastic Elastomer
A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4390 is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set ..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 4445 Thermoplastic Elastomer
A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4445 is a low hardness grade possessing exceptional tensile strength, superior compression s..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 4455 Thermoplastic Elastomer
A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4455 is a low hardness grade possessing exceptional tensile strength, superior compression s..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 4475 Thermoplastic Elastomer
A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4475 is a medium hardness grade possessing exceptional tensile strength, superior compressio..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 4480 Thermoplastic Elastomer
A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4480 is a medium hardness grade possessing exceptional tensile strength, superior compressio..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 3140 Thermoplastic Elastomer
A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3140 can be processed by injection molding or extrusion for appl..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 3480 Thermoplastic Elastomer
A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 3490 Thermoplastic Elastomer
A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 4139D Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4139D is a high hardness grade possessing exceptional tensile strength, superior compression set, chemical re..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 4339D Thermoplastic Elastomer
A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4339D is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set ..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Average value: 35.0 °C Grade Count:4
Overview of materials for PVC, Wire and Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 3180 Thermoplastic Elastomer
A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3180 can be processed by blow molding injection molding or ex..
Roll Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Extrusion
Teknor Apex Sarlink® 4149D Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4149D is a high hardness grade possessing exceptional tensile strength, superior compression set, chemical re..