Polymer Property : Roll Temperature = 180 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Roll Temperature 180 - 220 °C
356 - 428 °F
Hotmelt Coating Multi Roller
EMS-Griltech Griltex® 6E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Roll Temperature 180 - 220 °C
356 - 428 °F
Engraved Roller
EMS-Griltech Griltex® 9E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Roll Temperature 180 - 220 °C
356 - 428 °F
Engraved Roller
EMS-Griltech Griltex® D 1299A Heat Stabilized Copolyamide Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Roll Temperature 180 - 220 °C
356 - 428 °F
Hotmelt Coating Multi Roller
EMS-Griltech Griltex® D 1377E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Roll Temperature 180 - 220 °C
356 - 428 °F
Hotmelt Coating Multi Roller
EMS-Griltech Griltex® D 1439E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Roll Temperature 180 - 220 °C
356 - 428 °F
Engraved Roller
EMS-Griltech Griltex® D 1441E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Roll Temperature 180 - 220 °C
356 - 428 °F
Engraved Roller
EMS-Griltech Griltex® D 1500A Copolyamide Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Roll Temperature 180 - 220 °C
356 - 428 °F
Engraved Roller
EMS-Griltech Griltex® D 1516A Heat Stabilized Copolyamide Hotmelt Adhesive (Technical Applications)
GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides for excellent r..
Roll Temperature 180 - 230 °C
356 - 446 °F
Hotmelt Coating Multi Roller
EMS-Griltech Griltex® D 1519E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Roll Temperature 180 - 220 °C
356 - 428 °F
Engraved Roller
EMS-Griltech Griltex® D 1531E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Roll Temperature 180 - 220 °C
356 - 428 °F
Engraved Roller
EMS-Griltech Griltex® D 1533E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Roll Temperature 180 - 220 °C
356 - 428 °F
Engraved Roller
EMS-Griltech Griltex® D 1539E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Roll Temperature 180 - 230 °C
356 - 446 °F
Hotmelt Coating Multi Roller
EMS-Griltech Griltex® D 1619E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..