Processing Properties | Metric | English | Comments |
---|---|---|---|
Recrystallization Temperature | 2000 °C | 3630 °F | Deformation level - 99.99% |
Plansee ML Molybdenum-Lanthanum Oxide Characteristics:"Stacked fiber" microstructureExtremely creep resistantApplications:Furnace components - wires, including stranded; sintering and annealing boats; evaporator coilsLighting - retainin.. |
|||
Recrystallization Temperature | 2000 °C | 3630 °F | Deformation level - 99.99% |
Plansee WVM Potassium-doped Tungsten Doping tungsten with potassium and subjecting the material to a highly orientation-dependant cold working produces a stacked microstructure, yielding useful characteristics in wire and rod products.. |