Processing Properties Metric English Comments
Cure Time 8.00 - 16.0 min
0.133 - 0.267 hour
t'90; ASTM D2084 (mod)
ExxonMobil Chlorobutyl 1066 Rubber
Product Description: Exxon™ Chlorobutyl rubber is a copolymer of isobutylene and isoprene. The product has characteristic specific gravity of 0.93. The product form is white to light amber bales.In..
Cure Time 10.0 - 16.0 min
0.167 - 0.267 hour
t`90; ASTM D2084
ExxonMobil Exxon™ 5066 Chlorinated Star-Branched Butyl
Exxon Chloromobutyl is a chlorinated copolymer of isobutylene and isoprene.Information provided by ExxonMobil Chemical