Cure Time 10.0 - 15 min
0.167 - 0.25 hour
Gwent Electronic Materials C2000107P3 Silver Ink
Silver Ink C2000107P3 is designed as a termination for single layer PZT ceramics. After firing the film has good adhesion and solderability.The ink is in a ready to use form at a viscosity suitable..
Cure Time 7.98 - 15 min
0.133 - 0.25 hour
Gwent Electronic Materials C2000808D2 Silver Backlight Ink
Silver Ink C2000808D2 is a high resistance ink designed for use as the heating bars and tracks on automobile backlights and other circuits on glass. It has dark color when printed and fired on floa..
Cure Time 10.0 - 15 min
0.167 - 0.25 hour
Gwent Electronic Materials C2010829D2 Silver Ink
Silver Ink C2010829D2 is a high definition silver ink for LTCC tape. It is compatible with other members of the GEM range of Silver LTCC Inks and most LTCC tape systems on the market.The ink has be..
Cure Time 10.0 - 15 min
0.167 - 0.25 hour
Gwent Electronic Materials C2010515D4 Silver Ink
Silver Ink C2010515D4 is designed as an internal electrode ink for LTCC applications. It is compatible with other members of the GEM range of Silver LTCC Inks and most LTCC tape systems on the mark..
Cure Time 10.0 - 15 min
0.167 - 0.25 hour
Gwent Electronic Materials C2031105D2 Palladium Ink
Palladium Ink C2031105D2 is an ink formulated for screen printing for use on Fuel Cells. It is suitable for application onto Solid Oxide Fuel Cells.The ink has been made at a ready to use viscosity..
Cure Time 10 - 15 min
0.17 - 0.25 hour
Fixture
Loctite® 3035™ Polyolefin Bonder
Loctite® 3035™ Polyolefin Bonder is an easy-to-use, 1:1 mix product that can be stored at room temperature and works where traditional low surface energy bonders often fail. Loctite® 3035™ Polyo..
Cure Time 10.0 - 15 min
0.167 - 0.25 hour
Gwent Electronic Materials C2010809D3 Silver Ink
Silver Ink C2010809D3 is designed for printing via, when screen printed onto LTCC tape. It is compatible with other members of the GEM range of Silver LTCC Inks and most LTCC tape systems on the ma..