Cure Time 12.0 - 14.0 min
0.200 - 0.233 hour
Working time
ITW Devcon Metal Welderâ„¢ Methacrylate Adhesive II, Grey / Beads
Information provided by ITW Devcon
Cure Time 6.00 - 14.0 min
0.100 - 0.233 hour
t`90; ASTM D2084
ExxonMobil Exxon™ 2222 Regular Cure Rate Grade
Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product for is white to light amber bales.Information provided by ExxonMobil Chemical
Cure Time 6.00 - 14.0 min
0.100 - 0.233 hour
t`90; ASTM D2084
ExxonMobil Exxon™ 2235 Regular Cure Rate Grade
Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product form is white to light amber bales.Information provided by ExxonMobil Chemical
Cure Time 6.00 - 14.0 min
0.100 - 0.233 hour
t`90; ASTM D2084
ExxonMobil Exxon™ 2255 Regular Cure Rate Grade
Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene.The product form is white to light amber bales.Information provided by ExxonMobil Chemical
Cure Time 8.00 - 14.0 min
0.133 - 0.233 hour
t`90; ASTM D2084
ExxonMobil Exxon™ 6222 Brominated Star-Branched Butyl
Exxon SB Bromobutyl is a brominated copolymer of isobutylene and isoprene, including a styrene block copolymer branching agent.Information provided by ExxonMobil Chemical