Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 2.50 - 5.83 min | 0.0417 - 0.0972 hour | Gelation time |
Mitsui MILEX™ XL-1210MB Phenol Aralkyl Resin, Silicone Rubber Modified
(discontinued **) The MILEX™ Family of products is widely featured in brake systems of automobiles made by the top automakers through Mitsui Chemicals' affiliation with leading brake manufacturers. The phenolic .. |