Polymer Property : Cure Time = 0.0670 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 3 - 4.02 min
0.05 - 0.0670 hour
Demold Time
ACC EP IS EPI Engineered Polymers Integral Skin Flexible Foam
EP-IS is integral skin flexible foam, “Powered by Reactamine ® Technology”, designed to give excellent surface skin. EP-IS contains cyclopentane as its blowing agent, which conforms to EPA standa..