Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 0.500 - 1.17 min | 0.00833 - 0.0195 hour | Dry Time |
Loctite® 7649 Acetone Base Primer N Surface PreparersLoctite offers a complete line of surface preparation products to ensure the maximum performance of Loctite® Adhesives and Sealants.Loctite® Accelerators are used to increase the .. |
|||
Cure Time | 0.333 - 1.17 min | 0.00555 - 0.0195 hour | Time to Handling Strength |
3M Scotch-Weld™ LO1000 Low Odor Instant Adhesive 3M™ Scotch-Weld™ Low-Odor Instant Adhesives are formulated to have low volatility while maintaining bonding of a wide rage of materials. Low volatility means that these products are not only low o.. |
|||
Cure Time | 0.500 - 1.17 min | 0.00833 - 0.0195 hour | Dry Time |
Loctite® 7471 Acetone/Isopropanol Base Primer T Surface PreparersLoctite offers a complete line of surface preparation products to ensure the maximum performance of Loctite® Adhesives and Sealants.Loctite® Accelerators are used to increase the .. |