Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 0.167 - 0.500 min | 0.00278 - 0.00833 hour | On Steel (Fixture) |
ND Industries SuperGlue Ethyl 320 Very low viscosity for pre-assembled componentsMeets military spec Mil-A-46050C Type II Class I |
|||
Cure Time | 0.417 - 0.500 min | 0.00694 - 0.00833 hour | Steel, set time, cured |
Permabond 738 Cyanoacrylate, toughened PERMABOND 738 is a toughened cyanoacrylate with improved impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable over.. |
|||
Cure Time | 0.167 - 0.500 min | 0.00278 - 0.00833 hour | fixture time with initiator 43 |
Permabond TA439 Toughened Acrylic Adhesive Permabond® TA439 is a two component structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some plastics. The typical fixture time of is 10-30 seconds. The fast f.. |
|||
Cure Time | 0.250 - 0.500 min | 0.00417 - 0.00833 hour | zinc, fixture time with initiator 43 |
Permabond TA459 Toughened Acrylic Adhesive Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sens.. |
|||
Cure Time | 0.250 - 0.500 min | 0.00417 - 0.00833 hour | zinc, fixture time with initiator 44 |
Permabond TA4590 Toughened Acrylic Adhesive Permabond TA4590 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sen.. |
|||
Cure Time | 0.167 - 0.500 min | 0.00278 - 0.00833 hour | zinc, Fixture time |
Permabond TA4592 Toughened Acrylic Adhesive PERMABOND® TA4592 is a two component structural acrylic adhesive ideal for bonding magnets and ferrites for electric motors on fast-moving production lines. Permabond® TA4592 provides high strengt.. |
|||
Cure Time | 0.167 - 0.500 min | 0.00278 - 0.00833 hour | under visible/UV light |
Hybrid Plastics NanoBondâ„¢ UV Curable Adhesive Generally used for dental and optical applications.Information provided by Hybrid Plastics |
|||
Cure Time | 0.167 - 0.500 min | 0.00278 - 0.00833 hour | 350-380nm |
Tra-Con Tra-Bond 546S01 Low Viscosity UV Curable Adhesive TRA-BOND 546S01 is a low viscosity UV curable adhesive with a secondary heat curing system to achieve a high Tg. It exhibits excellent adhesion to glass and many other substrates, making it ideal fo.. |
|||
Cure Time | 0.330 - 0.500 min | 0.00550 - 0.00833 hour | Dry Time |
Loctite® 7644 Decafluoropentane Base Surface Primer Surface PreparersLoctite offers a complete line of surface preparation products to ensure the maximum performance of Loctite® Adhesives and Sealants.Loctite® Accelerators are used to increase the .. |
|||
Cure Time | 0.333 - 0.500 min | 0.00556 - 0.00833 hour | per mm |
Amity Thermosets ATF 197 Phenolic Molding Inorganic and glass Filler, Compression Molded Characteristics:Flame retardantSpark resistant Good electrical insulationHeat stability ( 200°C )Good mouldability Low water absorptionLow shrinkageColor-blackSoft/medium flow Applications:Switchg.. |
|||
Cure Time | 0.333 - 0.500 min | 0.00556 - 0.00833 hour | per mm |
Amity Thermosets ATI 172 Phenolic Molding Organic and inorganic Filler, Injection Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackVery soft flow .. |
|||
Cure Time | 0.333 - 0.500 min | 0.00556 - 0.00833 hour | per mm |
Amity Thermosets ATS 166 Phenolic Molding Chopped cotton fabric Filler, Compression Molded Characteristics:High impact strengthGlossy surfaceLow shrinkageGood sliding propertiesColor-BlackMedium flowApplications:Cog wheelsCastor wheelsBush bearingsPulleysWelding rod handlesTextile bobbins.. |
|||
Cure Time | 0.167 - 0.500 min | 0.00278 - 0.00833 hour | Time to Handling Strength |
3M Scotch-Weld™ EC40 General Purpose Instant Adhesive 3M™ Scotch-Weld™ General Purpose Instant Adhesives are single component, high strength ethyl cyanoacrylate adhesive designed to bond to a variety of substances including most plastics, rubbers, me.. |
|||
Cure Time | 0.167 - 0.500 min | 0.00278 - 0.00833 hour | Time to Handling Strength |
3M Scotch-Weld™ PR100 Plastic and Rubber Instant Adhesive 3M™ Scotch-Weld™ Plastic and Rubber Instant Adhesive is designed to give exceptional performance on difficult-to-bond plastic and rubber substrates. This adhesive may be bonded to like substrates .. |
|||
Cure Time | 0.016666 - 0.500 min | 0.00027777 - 0.00833 hour | |
3M Scotch-Weld™ CA7 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Very fast setting and excellent adhesion to metals, plastics, and rubbers.Information provided by 3.. |
|||
Cure Time | 0.333 - 0.500 min | 0.00556 - 0.00833 hour | per mm |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Compression Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft/medium flow Applications:Telecommuni.. |
|||
Cure Time | 0.0500 - 0.500 min | 0.000833 - 0.00833 hour | Time to Handling |
3M Scotch-Weld™ MG100 SF Medical Grade Instant Adhesive 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti.. |
|||
Cure Time | 0.333 - 0.500 min | 0.00556 - 0.00833 hour | per mm |
Amity Thermosets ATS 766 Phenolic Molding Chopped cotton fabric Filler, Compression Molded Characteristics:High impact strengthGlossy surfaceLow shrinkageGood sliding propertiesColor-BrownMedium flowApplications:Cog wheelsCastor wheelsBush bearingsPulleysWelding rod handlesTextile bobbins.. |
|||
Cure Time | 0.0500 - 0.500 min | 0.000833 - 0.00833 hour | Time to Handling |
3M Scotch-Weld™ MG20 SF Medical Grade Instant Adhesive 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti.. |
|||
Cure Time | 0.0500 - 0.500 min | 0.000833 - 0.00833 hour | Time to Handling Strength |
3M Scotch-Weld™ SF100 Super Fast Instant Adhesive 3M™ Scotch-Weld™ Super Fast Instant Adhesives rely less on surface moisture for cure speed than standard cyanoacrylates. They are designed to join together difficult-to-bond plastics and rubbers, .. |
|||
Cure Time | 0.0500 - 0.500 min | 0.000833 - 0.00833 hour | Time to Handling Strength |
3M Scotch-Weld™ SF20 Super Fast Instant Adhesive 3M™ Scotch-Weld™ Super Fast Instant Adhesives rely less on surface moisture for cure speed than standard cyanoacrylates. They are designed to join together difficult-to-bond plastics and rubbers, .. |
|||
Cure Time | 0.333 - 0.500 min | 0.00556 - 0.00833 hour | Steel, handling time |
Permabond 947 Cyanoacrylate, low odor PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |