Processing Properties Metric English Comments
Cure Time 2520 min
42.0 hour
Tack-Free Time
3M AC-275 Class B-4 Aerospace Sealant
3M Aerospace Sealant AC-275 Class B is a high temperature two-component manganese dioxide cured, liquid polysulfide polymer sealants providing excellent fuel tank and fuselage seals. They have outst..