Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 240 min | 4.00 hour | On steel (fixture) |
ND Industries 420 Instant High Pressure Pipe Sealant Industrial grade, controlled locking strength for metal fittings |
|||
Cure Time | 240 min | 4.00 hour | Full cure |
Resinlab® CYNERGY CA6301 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Cure Time | 240 min | 4.00 hour | Full cure |
Resinlab® CYNERGY CA6308 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Cure Time | 240 min | 4.00 hour | |
Lord Adhesives 320 Toughened, High Viscosity SMC, FRP, General Purpose Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Cure Time | 240 min | 4.00 hour | Fixture time |
ITW Devcon Safety Clear Coatâ„¢ Epoxy, Water Clear Information provided by ITW Devcon |
|||
Cure Time | 240 min @Temperature 200 °C |
4.00 hour @Temperature 392 °F |
Post |
Shin-Etsu Silicones SV-16000U Silicone Rubber SV16000U is one of a series of easy processing, no post cure silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering. Product Feat.. |
|||
Cure Time | 240 min @Temperature 200 °C |
4.00 hour @Temperature 392 °F |
Post |
Shin-Etsu Silicones X-30-1028U Low Temperature Silicone Elastomer ShinEtsu X301028U is a phenyl (PVMQ) silicone base. This product is designed for good low temperature characteristics. Product Features: A broad range of service temperatures from 100 to +260°C (.. |
|||
Cure Time | 240 min @Temperature 200 °C |
4.00 hour @Temperature 392 °F |
Post |
Shin-Etsu Silicones KE-167U Low Temperature Silicone Elastomer ShinEtsu KE167U is a phenyl (PVMQ) silicone compound. This product is designed for good low temperature characteristics.Product Features: A broad range of service temperatures from 100 to +260°C .. |
|||
Cure Time | 240 min @Temperature 200 °C |
4.00 hour @Temperature 392 °F |
Post |
Shin-Etsu Silicones KE-5530U Low Temperature Silicone Elastomer ShinEtsu KE5530 U is a nominal 30 Durometer phenyl (PVMQ) base.Product Features: This material was designed for its excellent vibration dampening characteristics. Because of its phenyl content, it a.. |
|||
Cure Time | 240 min @Temperature 200 °C |
4.00 hour @Temperature 392 °F |
Post |
Shin-Etsu Silicones KE-5550U Low Temperature Silicone Elastomer ShinEtsu KE5550 U is a nominal 50 Durometer phenyl (PVMQ) base.Product Features: This material was designed for its excellent vibration dampening characteristics. Because of its phenyl content, it a.. |
|||
Cure Time | 240 min @Temperature 200 °C |
4.00 hour @Temperature 392 °F |
Post |
Shin-Etsu Silicones KE-5570U Low Temperature Silicone Elastomer ShinEtsu KE5570 U is a nominal 70 Durometer phenyl (PVMQ) base.Product Features: This material was designed for its excellent vibration dampening characteristics. Because of its phenyl content, it a.. |
|||
Cure Time | 240 min @Temperature 200 °C |
4.00 hour @Temperature 392 °F |
Post |
Shin-Etsu Silicones KE-7022U Temperature Resistant Silicone Elastomer KE7022 U is intended for applications where excellent high heat resistance is required.Product Features: This product is intended for high temperature service as 55 ~+ 300 °C(67 ~ +570 °F).Typ.. |
|||
Cure Time | 240 min @Temperature 200 °C |
4.00 hour @Temperature 392 °F |
Post |
Shin-Etsu Silicones KE-9610U Silicone Elastomer KE9610 U is one of a series of easy processing, general purpose silicone rubber base with low volatile content. It can be used in a variety of applications requiring finishing by molding, extruding .. |
|||
Cure Time | 240 - 480 min @Temperature 23.0 °C |
4.00 - 8.00 hour @Temperature 73.4 °F |
|
Master Bond EP77M-F Silver Conductive, Fast Curing Epoxy Adhesive Master Bond Polymer System EP77M-F is a two component, silver filled, electrically conductive adhesive for high performance bonding formulated to cure very rapidly at room temperature. Unlike the ma.. |
|||
Cure Time | >= 240 min | >= 4.00 hour | |
Trelleborg Emerson & Cuming Stycast® 2651-1 One-Component Epoxy High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Cure Time | 240 - 1440 min | 4.00 - 24.0 hour | Full Cure Time @ 20ºC |
Loctite® Output™ 315 Acrylic Adhesive Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or.. |
|||
Cure Time | 240 min @Temperature 121 °C |
4.00 hour @Temperature 250 °F |
|
Cotronics 4700 Ultra Temp Adhesive and Casting Epoxy, General Purpose |
|||
Cure Time | 240 min | 4.00 hour | Tack-Free Time |
3M AC-251 Black Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-251 Black Class B are two-part, quick curing, polysulfide based canopy and windshield sealants. These products are formulated for sealing acrylic, glass, and polycarbonate ai.. |
|||
Cure Time | 240 - 360 min | 4.00 - 6.00 hour | Tack Free Time, catalyzed with QM CAT PURPLE |
ACC QM 122 QSI Quantum Silicones 22 Durometer Condensation Cured Moldmaking Material QM 122 is a two-component, room temperature condensation cure silicone material. The cured rubber is flexible with excellent mechanical and physical properties in addition to good shelf-life stabili.. |
|||
Cure Time | 240 - 360 min | 4.00 - 6.00 hour | Tack Free Time, catalyzed with QM CAT 140 |
ACC QM 140 QSI Quantum Silicones 40 Durometer Condensation Cured Moldmaking Material QM 140 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent cho.. |
|||
Cure Time | 240 min | 4.00 hour | Touch Dry |
3M Scotchkote™ MC 145 Epoxy Primer Scotchkote Epoxy Primer MC 145 is a solvent based two component primer suitable for use on a wide range of metallic and glass reinforced plastic (GRP) surfaces prior to the application of Scotchkote.. |
|||
Cure Time | 240 - 1440 min | 4.00 - 24.0 hour | Full cure |
3M Scotch-Weld™ DP812 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP812 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and.. |
|||
Cure Time | 240 min | 4.00 hour | Touch Dry |
3M Scotchkote™ 445 Epoxy Slip Deterrent System Scotchkote Epoxy Slip Deterrent System 445 has been specifically developed as a 100% solids system for use with 3M Scotchkote Granular Aggregate to provide a slip deterrent finish to high risk floor.. |
|||
Cure Time | 240 - 360 min | 4.00 - 6.00 hour | Tack Free Time, catalyzed with Moldmaster Green |
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Cure Time | 240 min | 4.00 hour | Tack-free time |
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M |
|||
Cure Time | 240 - 480 min | 4.00 - 8.00 hour | Mixture reaches handling strength in 4 to 8 hours. |
Fibre Glast 88 / 87 General Purpose Epoxy Resin and Hardener
(discontinued **) Description:#88 Epoxy Resin is a 100% reactive low viscosity liquid bisphenol-A based epoxy resin diluted with Alkyl glycidyl ether. This resin is specially designed for applications requiring low v.. |