Processing Properties Metric English Comments
Cure Time 2160 - 2880 min
36.0 - 48.0 hour
90% of maximum strength developed within
Master Bond EP21TDCN Two Component Nickel Conductive Epoxy Adhesive
Product Description: Master Bond Polymer System EP21TDCN is a two component, nickel filled, electrically conductive, adhesive for high performance bonding, formulated to cure at room temperature or ..
Cure Time 2160 min

@Temperature 22.0 °C
36.0 hour

@Temperature 71.6 °F
Dow Corning 748 NON-CORROSIVE SEALANT
White, neutral cure RTV sealant especially for electrical applications.Information provided by Dow Corning