Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 60.0 min | 1.00 hour | On steel (fixture) |
ND Industries StudGrade® 146 Permanent StudGrade HD Threadlocker General DescriptionHigh strength, high viscosity threadlockers for maximum security. Suitable for most applications where disassembly is not required.Typical UsesFasteners over 1" diameter with coa.. |
|||
Cure Time | 60.0 min | 1.00 hour | Cure for Service |
Protective Coating PC-Plumbing Epoxy Putty™ Hand Moldable, Multi-Purpose Epoxy Putty Stick Description: After Mixing, PC-Plumbing™ can be used to repair split and leaking pipes, tanks, drums, castings, ducts, valves and tools. It can be used wherever metal is missing, dented, broken, or .. |
|||
Cure Time | 60.0 - 180 min | 1.00 - 3.00 hour | Functional |
Palm Labs Adhesives TURBO-LOCK SERIES 10 Anaerobic Thread Locking Compound TURBO-LOCK SERIES 10 is a removable, PURPLE, fast curing, low strength, anaerobic thread-locking compound for bonding and sealing small screw threads. It is highly resistance to heat, vibrations, wa.. |
|||
Cure Time | 60.0 - 180 min | 1.00 - 3.00 hour | Functional |
Palm Labs Adhesives TURBO-LOCK SERIES 13-OR Anaerobic Thread Locking Compound TURBO-LOCK 13-OR SERIES is a RED, high temperature, high strength, permanent, oil resistant, anaerobic thread-locking compound. It is highly resistance to heat, vibrations, water, gases, oils, hydro.. |
|||
Cure Time | <= 60.0 min @Temperature 185 °C |
<= 1.00 hour @Temperature 365 °F |
Paint Cure Cycle; Chomerics |
Parker Chomerics CHO-MASK II ST Conductive Foil Tape The CHO-MASK II family of EMI foil tapes includes both Standard Tack (ST) and High Tack (HT) versions for providing a conductive, non-corroding surface on painted metal electronic enclosures. CHO-MA.. |
|||
Cure Time | 60.0 min @Temperature 121 °C |
1.00 hour @Temperature 250 °F |
|
Parker Chomerics CHO-SHIELD® 611 Part A Conductive Coating Comments: Variant of CHO-SHIELD 596Typical Applications:Protecting EMI flangesInformation provided by Chomerics |
|||
Cure Time | 60.0 - 180 min | 1.00 - 3.00 hour | Functional |
Palm Labs Adhesives TURBO-LOCK SERIES 16 Anaerobic Thread Locking Compound TURBO-LOCK SERIES 16 is a fast curing, GREEN, medium strength, wicking grade, anaerobic thread-locking compound for bonding and sealing threads, and pre-assembled parts. It is highly resistance to h.. |
|||
Cure Time | 60.0 - 180 min | 1.00 - 3.00 hour | Functional |
Palm Labs Adhesives TURBO-LOCK SERIES 17-GP Anaerobic Thread Locking Compound BEARING AND SHAFT - SERIES 17-GP is a fast curing, GREEN, high strength, general purpose, press fit, anaerobic retaining compound for bonding, sealing and retaining of cylindrical parts. It is highl.. |
|||
Cure Time | 60.0 min @Temperature 142 °C |
1.00 hour @Temperature 287 °F |
|
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Cure Time | 60.0 min @Temperature 142 °C |
1.00 hour @Temperature 287 °F |
|
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Cure Time | 60.0 min @Temperature 121 °C |
1.00 hour @Temperature 250 °F |
|
Henkel Hysol EA 9628H Film Adhesive First generation, modified epoxy film, high peel strength, good stress, environmental resistance and structural propertiesApplications: Composite Bonding, Metal & Honeycomb BondingData from .060 psf.. |
|||
Cure Time | 60.0 min @Temperature 177 °C |
1.00 hour @Temperature 351 °F |
|
Henkel Hysol EA 9673 (BMI) Film Adhesive Modified BMI film adhesive, superior strength to 550°F / 288°C. Moisture resistant, processes like conventional high temperature epoxies. Minimum order required. Data from 0.10 psf, 500 g / m2.. |
|||
Cure Time | 60.0 min @Temperature 95.0 °C |
1.00 hour @Temperature 203 °F |
|
Tra-Con Tra-Bond 957-1R Polyurethane Adhesive TRA-BOND 957-1R is a polyurethane compound used on stress sensitive components and encapsulation applications. Information provided by Tra-Con Inc. |
|||
Cure Time | 60.0 min @Temperature 142 °C |
1.00 hour @Temperature 287 °F |
|
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Cure Time | 60.0 min @Temperature 142 °C |
1.00 hour @Temperature 287 °F |
|
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Cure Time | 60.0 min @Temperature 150 °C |
1.00 hour @Temperature 302 °F |
|
Dow Corning JCR 6126 W/C Two-part, translucent, thixotropic, medium modulus LED encapsulant with a very long working time.Information provided by Dow Corning |
|||
Cure Time | 60.0 min @Temperature 150 °C |
1.00 hour @Temperature 302 °F |
|
Epoxy Technology EPO-TEK® 337H Graphite-Filled, High Temperature Epoxy Product Description: EPO-TEK® 377H is a two component, high Tg, graphite filled epoxy designed for ESD/EMI shielding of semiconductor devices and electronics. It can be used in many electronic ind.. |
|||
Cure Time | 60.0 min @Temperature 180 °C |
1.00 hour @Temperature 356 °F |
Minimum Bond Line |
Epoxy Technology EPO-TEK® E3035T-2 Electrically Conductive Epoxy Product Description: EPO-TEK® E3035T-2 is a single component, silver-filled epoxy for semiconductor die attach, as well as SMD attach on hybrid circuits.Advantages & Application Notes: This epoxy c.. |
|||
Cure Time | 60.0 min @Temperature 150 °C |
1.00 hour @Temperature 302 °F |
|
Dow Corning EG-3000 THIXOTROPIC GEL PARTS A&B Two-part, heat cure, thixotropic gel.Information provided by Dow Corning |
|||
Cure Time | >= 60.0 min | >= 1.00 hour | Air Set prior to curing |
Aremco Corr-Paint™ CP3015-GR High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Gray-ceramic inorganic coating to 1400°F. |
|||
Cure Time | 60.0 min | 1.00 hour | Full Cure |
3M Scotch-Weld™ DP601NS Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the compon.. |
|||
Cure Time | 60.0 - 120 min @Temperature 24.0 °C |
1.00 - 2.00 hour @Temperature 75.2 °F |
demold time |
BCC Products Kwik Kast BC 8001 Urethane Casting BC8001 is an advanced fast cast polyurethane tooling system. It features low viscosity, low exotherm and minimal shrinkage. It cures hard, yet more durable resulting in less brittle parts. Designed.. |
|||
Cure Time | >= 60.0 min | >= 1.00 hour | Air Set prior to curing |
Aremco Corr-Paint™ CP4020 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4010 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Cure Time | >= 60.0 min | >= 1.00 hour | Air Set prior to curing |
Aremco Corr-Paint™ CP4020-S1 High Temperature Protective Coating, Silicone |
|||
Cure Time | 60.0 min @Temperature 93.3 °C |
1.00 hour @Temperature 200 °F |
>0.5 Hour Air Set Required Prior to Curing |
Aremco Pyro-Paint™ 634-YO High Temperature Refractory Coating, YO >95% This ultra high temperature yttrium oxide coating provides exceptional protection of graphite, ceramic and metal components exposed to reactive molten metals such as titanium, uranium and their allo.. |
|||
Cure Time | 60.0 min @Temperature 142 °C |
1.00 hour @Temperature 287 °F |
|
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Cure Time | 60.0 min @Temperature 142 °C |
1.00 hour @Temperature 287 °F |
|
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Cure Time | 60.0 min @Temperature 142 °C |
1.00 hour @Temperature 287 °F |
|
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |