Processing Properties Metric English Comments
Cure Time 34.2 min

@Temperature 155 °C
0.570 hour

@Temperature 311 °F
TC90
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR Thanecure ZM
Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man..
Cure Time 34.2 min

@Temperature 155 °C
0.570 hour

@Temperature 311 °F
TC90
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR Thanecure ZM
Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man..