Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 20.0 min | 0.333 hour | On steel (fixture) |
ND Industries ScrewGrade® 111 Removable Threadlocker A low strength threadlocker which eliminates vibrational loosening, and seals against leakage and corrosion.Typical Usessoft metal fasteners, precision screws, and locking fasteners smaller than .25.. |
|||
Cure Time | 20.0 min | 0.333 hour | handling time, .5 mm gap |
Permabond TA435 Toughened Acrylic Adhesive & Initiator PERMABOND TA435 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This adhesive may be used in a variety of structural bonding appli.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 30 PHR N330 (HAF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 30 PHR N550 (FEF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR N990 (MT) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 50 PHR N774 (SRF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 50 PHR N990 (MT) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 70 PHR N774 (SRF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min | 0.333 hour | Dry Time to Handling; Fed Std 141 4061 |
Humiseal 1A33LSE Urethane Conformal Coating Humiseal 1A33LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses ther.. |
|||
Cure Time | 20.0 min | 0.333 hour | Dry Time to Handling; Fed Std 141 4061 |
Humiseal 1B73LSE Acrylic Conformal Coating Humiseal 1B73LSE Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityUL Approval PendingMIL-I-46058C Approval Pendin.. |
|||
Cure Time | 20.0 min @Temperature 150 °C |
0.333 hour @Temperature 302 °F |
|
Lord Adhesives Circalokâ„¢ EP-937 Epoxy Board Level Encapsulant LORD Thermosetâ„¢ EP-937 encapsulant is a black, one-component epoxy specifically designed to meet the needs of coating semiconductor devices on printed circuit boards.All information provided by.. |
|||
Cure Time | 20.0 min | 0.333 hour | Fixture time |
ITW Devcon 10 minuteâ„¢ Epoxy, Black Information provided by ITW Devcon |
|||
Cure Time | 20.0 min | 0.333 hour | Fixture time |
ITW Devcon 10 minuteâ„¢ Epoxy, Clear Information provided by ITW Devcon |
|||
Cure Time | 20.0 min | 0.333 hour | Tack-free |
Momentive Performance Materials RTV102 One Component Acetoxy Adhesive Sealant, White RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Cure Time | 20.0 min | 0.333 hour | Tack-free |
Momentive Performance Materials RTV103 One Component Acetoxy Adhesive Sealant, Black RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Cure Time | 20.0 min @Pressure 0.207 MPa, Temperature 40.0 °C |
0.333 hour @Pressure 30.0 psi, Temperature 104 °F |
|
Lucite International Colacryl ® TS 1649 Acrylic Orthodontic Polymer A range of methacrylate based copolymers designed for the manufacture of high quality orthodontic dental resins.Features: Excellent dry flow characteristics; Closely controlled particle size; Contai.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 50 PHR N774 (SRF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 70 PHR N330 (HAF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min @Temperature 154 °C |
0.333 hour @Temperature 310 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with Control Plasticizer MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 30 PHR N220 (ISAF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min | 0.333 hour | |
Loctite® 675 Medium Strength Retaining Compound RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. .. |
|||
Cure Time | 20.0 min @Temperature 154 °C |
0.333 hour @Temperature 310 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR Laminar Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min @Temperature 170 °C |
0.333 hour @Temperature 338 °F |
|
Dow BETAMATE™ 73345G Epoxy BETAMATE™ 73345G is a one-part, high performance, heat curing, epoxy adhesive. It is capable of bonding oily galvanized and cold rolled steel without a primer and has corrosion resistance. BETAMA.. |
|||
Cure Time | 20.0 min | 0.333 hour | Time to Handling Strength |
3M Scotch-Weld™ DP604NS Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesive DP-604NS is a black, rapid setting, two-component polyurethane. It is packaged as 1:1 ratio liquids in a duo-pak cartridge. With the squeeze of the trigger, the .. |
|||
Cure Time | <= 20.0 min | <= 0.333 hour | Fixture Time |
3M Scotch-Weld™ TL43 Threadlocker Anaerobic Adhesive 3M™ Scotch-Weld™ Threadlocker Anaerobic Adhesives are one-component anaerobic adhesives that cure and seal threaded assemblies that meet a wide range of applications to prevent vibration loosening.. |
|||
Cure Time | <= 20.0 min | <= 0.333 hour | Fixture Time |
3M Scotch-Weld™ TL62 Threadlocker Anaerobic Adhesive 3M™ Scotch-Weld™ Threadlocker Anaerobic Adhesives are one-component anaerobic adhesives that cure and seal threaded assemblies that meet a wide range of applications to prevent vibration loosening.. |
|||
Cure Time | <= 20.0 min | <= 0.333 hour | Fixture Time |
3M Scotch-Weld™ TL71 Threadlocker Anaerobic Adhesive 3M™ Scotch-Weld™ Threadlocker Anaerobic Adhesives are one-component anaerobic adhesives that cure and seal threaded assemblies that meet a wide range of applications to prevent vibration loosening.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 70 PHR N220 (ISAF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 20.0 min @Temperature 149 °C |
0.333 hour @Temperature 300 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR N220 (ISAF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |